Summary for Test 2019-01-28-6-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 213470
DEA: 06394604
EFIS: 0600020595
DIST-CO-RTE-PM06-FRE-269-10.6/12.4
Award Date11/02/2018
Closeout Date10/15/2020
Work DescriptionREPLACE BRIDGES AND RECONSTRUCT ROADWAY.
Location DescriptionFRESNO COUNTY NEAR HURON FROM 1.0 MILE NORTH OF PALMER AVENUE TO 0.4 MILE SOUTH OF ROUTE 198
QA Service Level1 (Verified on 09/25/2018)

Sample Information

Sample Taken Date01/28/2019 Sample Unique Key6
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing01/31/2019
Sample typeQuality Assurance A brief description of the samplebearing pad
The quantity of what the sample constitutes1 From where was the sample collectedManufacturer
First name of sampler or witnessed byKayla Last name of sampler or witnessed byWallace
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameDynamic Rubber Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)CR5500119
Material/Compound/Elastomer IDna Samples Representing11
Description (size)3.45" x 11" x 11" CommentsUnknown
Description (Number of Shims)6 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Dynamic Rubber
Batch Numberna

Test Details

DIME Sample ID: 2019-01-28-6
DIME Test ID: 2019-01-28-6-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2019-02-19

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steve
Date of test: 02/01/2019
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.067 in
Sample 1 Tear Strength: 209 lbf / in
Sample 2 Median Thickness: 0.064 in
Sample 2 Tear Strength: 218.8 lbf / in
Sample 3 Median Thickness: 0.066 in
Sample 3 Tear Strength: 227.3 lbf / in
UTM: no data
Median of the Tear Strength Values: 218.8 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 2/12/2019