Summary for Test 2018-05-14-11-3
Test performed: ASTM D624-00-re12Project Information
Project Identifiers | DEA: No Project |
---|---|
DIST-CO-RTE-PM | --- |
Award Date | Not set |
Closeout Date | 11/01/2022 |
Work Description | Special project identifier for material not associated with a project |
Location Description | Not set |
QA Service Level | NOT VERIFIED |
Sample Information
Sample Taken Date | 05/14/2018 | Sample Unique Key | 11 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 05/14/2018 |
Sample type | Quality Assurance | A brief description of the sample | .25in Bearing Pad Roll Stock |
The quantity of what the sample constitutes | 1 | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | Christy | Last name of sampler or witnessed by | Stockton |
Title of sampler | Unknown | Telephone number of sampler | Unknown |
Laboratory sample identification | Unknown | Linked DIME Sample ID | Unknown |
The fabricator/manufacturer/facility name | Scougal Rubber | Transportation Laboratory (TL) Number | Unknown |
Inspector Lot Number from the Transportation Laboratory (TL) Form | Unknown | Structure unique identifier | Not set |
Structure name | Not set |
Material Information
Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 1609785 |
---|---|---|---|
Material/Compound/Elastomer ID | Unknown | Samples Representing | 1 |
Description (size) | .25in x 12in x 12in | Comments | Unknown |
Description (Number of Shims) | 0 | Type of Bearing Pad | Plain |
Description (Thickness of Shims) | NA | Manufacturer(s) | Scougal Rubber |
Batch Number | Unknown |
Test Details
DIME Sample ID: 2018-05-14-11
DIME Test ID: 2018-05-14-11-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2018-05-28
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 05/17/2018
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.064 in
Sample 1 Tear Strength: 285.9 lbf / in
Sample 2 Median Thickness: 0.06 in
Sample 2 Tear Strength: 308.3 lbf / in
Sample 3 Median Thickness: 0.073 in
Sample 3 Tear Strength: 297.3 lbf / in
UTM: no data
Median of the Tear Strength Values: 297.3 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 5/21/2018 ✔