Summary for Test 2019-06-12-1-4

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 211260
DEA: 072159U4
EFIS: 0715000160
DIST-CO-RTE-PM07-LA,ORA-5-0.0/1.5, 44.3/44.4
Award Date05/27/2016
Closeout Date08/01/2023
Work DescriptionCONSTRUCT HOV LANES AND MIX FLOW LANES.
Location DescriptionLOS ANGELES AND ORANGE COUNTIES IN BUENA PARK, LA MIRADA, CERRITOS AND SANTA FE SPRINGS FROM ARTESIA BOULEVARD UNDERCROSSING TO NORTH FORK COYOTE CREEK
QA Service Level1 (Verified on 03/16/2016)

Sample Information

Sample Taken Date06/12/2019 Sample Unique Key1
Date that the sample was received by the laboratory/organization performing the testing06/19/2019 Sample typeDepartment Acceptance
A brief description of the sample13x13x2.5 Elastomeric Bearing Pad The quantity of what the sample constitutes2
From where was the sample collectedManufacturer First name of sampler or witnessed byKevin
Last name of sampler or witnessed byMuser Title of samplerQA
Telephone number of sampler9165170532 Laboratory sample identification
Linked DIME Sample ID The fabricator/manufacturer/facility nameScougal Rubber
Transportation Laboratory (TL) Number Inspector Lot Number from the Transportation Laboratory (TL) FormS19-185-19
Structure unique identifier Structure name
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)17920-1
Material/Compound/Elastomer ID55 Duro Samples Representing2
Description (size)13x13x2.5 CommentsUnknown
Description (Number of Shims)5 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch Number17920-1

Test Details

DIME Sample ID: 2019-06-12-1
DIME Test ID: 2019-06-12-1-4
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2019-06-26

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steve
Date of test: 06/21/2019
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.065 in
Sample 1 Tear Strength: 184.6 lbf / in
Sample 2 Median Thickness: 0.066 in
Sample 2 Tear Strength: 181.8 lbf / in
Sample 3 Median Thickness: 0.071 in
Sample 3 Tear Strength: 183.1 lbf / in
UTM: no data
Median of the Tear Strength Values: 183.1 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 6/26/2019