Summary for Test 2019-01-28-6-3
Test performed: ASTM D624-00-re12Project Information
| Project Identifiers | Project ID: 213470 DEA: 06394604 EFIS: 0600020595 |
|---|---|
| DIST-CO-RTE-PM | 06-FRE-269-10.6/12.4 |
| Award Date | 11/02/2018 |
| Closeout Date | 10/15/2020 |
| Work Description | REPLACE BRIDGES AND RECONSTRUCT ROADWAY. |
| Location Description | FRESNO COUNTY NEAR HURON FROM 1.0 MILE NORTH OF PALMER AVENUE TO 0.4 MILE SOUTH OF ROUTE 198 |
| QA Service Level | 1 (Verified on 09/25/2018) |
Sample Information
| Sample Taken Date | 01/28/2019 | Sample Unique Key | 6 |
|---|---|---|---|
| Date that the sample was received by the laboratory/organization performing the testing | 01/31/2019 | Sample type | Quality Assurance |
| A brief description of the sample | bearing pad | The quantity of what the sample constitutes | 1 |
| From where was the sample collected | Manufacturer | First name of sampler or witnessed by | Kayla |
| Last name of sampler or witnessed by | Wallace | Title of sampler | |
| Telephone number of sampler | Laboratory sample identification | ||
| Linked DIME Sample ID | The fabricator/manufacturer/facility name | Dynamic Rubber | |
| Transportation Laboratory (TL) Number | Inspector Lot Number from the Transportation Laboratory (TL) Form | ||
| Structure unique identifier | Not set | Structure name | Not set |
| Bid Item | Not set |
Material Information
| Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | CR5500119 |
|---|---|---|---|
| Material/Compound/Elastomer ID | na | Samples Representing | 11 |
| Description (size) | 3.45" x 11" x 11" | Comments | Unknown |
| Description (Number of Shims) | 6 | Type of Bearing Pad | Steel |
| Description (Thickness of Shims) | 14 gage | Manufacturer(s) | Dynamic Rubber |
| Batch Number | na |
Test Details
DIME Sample ID: 2019-01-28-6
DIME Test ID: 2019-01-28-6-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2019-02-19
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steve
Date of test: 02/01/2019
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.067 in
Sample 1 Tear Strength: 209 lbf / in
Sample 2 Median Thickness: 0.064 in
Sample 2 Tear Strength: 218.8 lbf / in
Sample 3 Median Thickness: 0.066 in
Sample 3 Tear Strength: 227.3 lbf / in
UTM: no data
Median of the Tear Strength Values: 218.8 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 2/12/2019 ✔