Summary for Test 2018-07-03-16-6

Test performed: CTM 670-December 2013

Project Information

Project Identifiers
DEA: No Project
DIST-CO-RTE-PM---
Award DateNot set
Closeout Date11/01/2022
Work DescriptionSpecial project identifier for material not associated with a project
Location DescriptionNot set
QA Service LevelNOT VERIFIED

Sample Information

Sample Taken Date07/03/2018 Sample Unique Key16
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing07/05/2018
Sample typeQuality Assurance A brief description of the sample size 7 flash welded hoops
The quantity of what the sample constitutes150 From where was the sample collectedFabricator
First name of sampler or witnessed bySteve Last name of sampler or witnessed byMorris
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameCMC Rebar Tracy CA Transportation Laboratory (TL) NumberUnknown
Inspector Lot Number from the Transportation Laboratory (TL) FormUnknown Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM5 - Welded Hoops Production or Authorization TestingAuthorization Testing
Service or UltimateUltimate Rebar Heat Number(s)4076299
Hoop Manufacturer Lot Number(s)1,5 Material Standard CodeASTM A706
Material Grade60 Rebar Size7
Diameter of Hoop3'-8" Epoxy CoatedNo
Epoxy Coating ColorNA Rebar ManufacturerCMC Etiwanda
Welding CompanyCMC Rebar (Tracy) Coating StandardsUncoated
Weld TypeFlash Welded

Test Details

DIME Sample ID: 2018-07-03-16
DIME Test ID: 2018-07-03-16-6
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: CTM 670-December 2013: Method of Tests for Mechanical and Welded Reinforcing Steel Splices (Tensile)
Test Release Date: 2018-07-16

Test Results


Number of Samples: 1
Input Type: Measured
Tester's full name: Brian
Date of test: 07/06/2018
UTM: 400KIP
Temperature: 72 F
NumSampleMfg. Lot Number(s)SizeArea (sqin)Peak Load (lbf)Peak Stress (psi)CommentsTested By
135#7/22mm0.65600093330Bar BrokeBrian

General comments (publicly viewable) (Max 1000 characters): Bar Broke; OK Necking
Test Graph
Source: Partner Data Point File
Test graph for the Sample

Test was verified on 7/9/2018