Summary for Test 2018-05-10-3-3

Test performed: ASTM D624-00-re12

Project Information

Project Identifiers
DEA: No Project
DIST-CO-RTE-PM---
Award DateNot set
Closeout Date11/01/2022
Work DescriptionSpecial project identifier for material not associated with a project
Location DescriptionNot set
QA Service LevelNOT VERIFIED

Sample Information

Sample Taken Date05/10/2018 Sample Unique Key3
Date that the sample was received by the laboratory/organization performing the testing05/14/2018 Sample typeQuality Assurance
A brief description of the sample.5in Bearing Pad Roll Stock The quantity of what the sample constitutes1
From where was the sample collectedManufacturer First name of sampler or witnessed byChristy
Last name of sampler or witnessed byStockton Title of samplerUnknown
Telephone number of samplerUnknown Laboratory sample identificationUnknown
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility nameWarco Biltrite Scougal Rubber
Transportation Laboratory (TL) NumberUnknown Inspector Lot Number from the Transportation Laboratory (TL) FormUnknown
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)4-9-18
Material/Compound/Elastomer IDNC 8168 Samples Representing1
Description (size).5in x 48in CommentsUnknown
Description (Number of Shims)0 Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)Warco Biltrite
Batch NumberNC 8168

Test Details

DIME Sample ID: 2018-05-10-3
DIME Test ID: 2018-05-10-3-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2018-05-28

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 05/17/2018
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.079 in
Sample 1 Tear Strength: 243 lbf / in
Sample 2 Median Thickness: 0.079 in
Sample 2 Tear Strength: 257 lbf / in
Sample 3 Median Thickness: 0.079 in
Sample 3 Tear Strength: 249.4 lbf / in
UTM: no data
Median of the Tear Strength Values: 249.4 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 5/21/2018 ✔