Summary for Test 2026-07-08-79-3

Test performed: ASTM D624-00r20

Project Information

Project IdentifiersProject ID: 994654
DEA: 07313504
EFIS: 0715000090
DIST-CO-RTE-PM07-LA,VEN-1-37.7/62.9,0.0/0.9
Award Date07/20/2023
Closeout DateNot set
Work DescriptionREMOVE AND CONSTRUCT BRIDGE AND CULVERTS.
Location DescriptionLOS ANGELES AND VENTURA COUNTIES AT VARIOUS LOCATIONS FROM 0.4 MILE SOUTH OF TEMESCAL CANYON ROAD TO 0.1 MILE NORTH OF TONGA STREET
QA Service Level1 (Verified on 07/24/2023)

Sample Information

Sample Taken Date07/08/2026 Sample Unique Key79
Will the laboratory/organization for which you are a member perform testing on this material sample?No Date that the sample was received by the laboratory/organization performing the testing07/20/2026
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutesX From where was the sample collectedManufacturer
First name of sampler or witnessed byKrishnamoorthy Last name of sampler or witnessed byPalaniappan
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameBridge Rubber Bearing Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifier
Structure name Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)2527-4
Material/Compound/Elastomer IDNA Samples Representing3
Description (size)1.15" x 8" x 12" Comments
Description (Number of Shims)2 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Bridge Rubber Bearing
Batch Number157119

Test Details

DIME Sample ID: 2026-07-08-79
DIME Test ID: 2026-07-08-79-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2026-08-06

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Andrew Auvinen
Date of test: 08/06/2026
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.069 in
Sample 1 Tear Strength: 234 lb/in
Sample 2 Median Thickness: 0.083 in
Sample 2 Tear Strength: 238 lb/in
Sample 3 Median Thickness: 0.073 in
Sample 3 Tear Strength: 232 lb/in
UTM: NA
Median of the Tear Strength Values: 234 lb/in
General comments (publicly viewable) (Max 1000 characters):

Test was verified on 8/6/2026