Summary for Test 2024-08-26-51-6
Test performed: AASHTO T308-10Project Information
| Project Identifiers | Project ID: 215003 DEA: 040J6204 EFIS: 0414000019 |
|---|---|
| DIST-CO-RTE-PM | 04-ALA-680-12.4/21.9 |
| Award Date | 04/12/2022 |
| Closeout Date | Not set |
| Work Description | REHABILITATE PAVEMENT - RPL APP/DEP SLABS, 14 BRIDGES |
| Location Description | ALAMEDA COUNTY AT SUNOL AND IN PLEASANTON AND DUBLIN FROM KOOPMANN ROAD UNDERCROSSING TO ALAMEDA COUNTY LINE |
| QA Service Level | 1 (Verified on 10/19/2020) |
Sample Information
| Sample Taken Date | 08/26/2024 | Sample Unique Key | 51 |
|---|---|---|---|
| Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 08/27/2024 |
| Sample type | Quality Assurance | A brief description of the sample | 1/2"RHMA-G |
| The quantity of what the sample constitutes | 750 Tons | From where was the sample collected | Source |
| First name of sampler or witnessed by | Bhalinder | Last name of sampler or witnessed by | Pandher |
| Title of sampler | Telephone number of sampler | ||
| Laboratory sample identification | Linked DIME Sample ID | ||
| The fabricator/manufacturer/facility name | Vulcan Pleasanton | Transportation Laboratory (TL) Number | C032310 |
| Inspector Lot Number from the Transportation Laboratory (TL) Form | Structure unique identifier | ||
| Structure name | Bid Item | Not set |
Material Information
| Material Type | Hot Mix Asphalt | HMA Type | Type A HMA |
|---|---|---|---|
| HMA Grading | 1/2 inch | Lot number | 1 |
| Sublot number | 1 | HMA Mix Number | 326122 |
| Binder content (%) | Not set | Virgin binder PG | Not set |
| Design binder PG | Not set | Binder Supplier | Not set |
| RAP content (%) | Not set | WMA Additives | Not set |
| Antistrip type | Not set |
Test Details
DIME Sample ID: 2024-08-26-51
DIME Test ID: 2024-08-26-51-6
Testing Lab: CT D04 - Pleasanton Field Laboratory
Test Method: AASHTO T308-10: Standard Method of Test for Determining the Asphalt Binder Content of Hot Mix Asphalt (HMA) by the Ignition Method (Method A) (Asphalt Binder Content)
Test Release Date: 2024-09-05
Test Results
What temperature unit is used?: Celsius
Input Type: Measured
Tester's full name: Robert Lohman
Date of test: 08/29/2024
Test procedure used?: Method A
Mass of the specimen basket assembly: 2900.2 g
Mass of the specimen and specimen basket assembly prior to ignition: 4494.9 g
Mass of HMA Sample prior to ignition: 1594.7 g
Mass Loss: 102.0 g
Mass of aggregate remaining after ignition: 1492.7 g
Correction Factor (Percent by mass of HMA Specimen): 0.55 %
Moisture Content: 0.00 %
Temperature Compensation Factor: 0.19 %
Test Temperature: 482 C
Corrected Asphalt Binder Content: 5.66 %
General comments (publicly viewable) (Max 1000 characters): Burn #1
Test was verified on 9/5/2024 ✔