Summary for Test 2019-03-07-4-3
Test performed: ASTM D624-00-re12Project Information
Project Identifiers | Project ID: 212993 DEA: 033F5304 EFIS: 0313000135 |
---|---|
DIST-CO-RTE-PM | 03-ED-50-67.3 |
Award Date | 11/09/2018 |
Closeout Date | 09/20/2022 |
Work Description | ECHO SUMMIT BRIDGE IS A 24-FT WIDE, THREE-SPAN, REINFORCED CONCRETE GIRDER BRIDGE |
Location Description | EL DORADO COUNTY NEAR MEYERS AT ECHO SUMMIT SIDEHILL VIADUCT |
QA Service Level | 1 (Verified on 01/08/2019) |
Sample Information
Sample Taken Date | 03/07/2019 | Sample Unique Key | 4 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 03/08/2019 |
Sample type | Quality Assurance | A brief description of the sample | Bearing Pad |
The quantity of what the sample constitutes | 1 | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | Pete | Last name of sampler or witnessed by | Etcheverry |
Title of sampler | Telephone number of sampler | ||
Laboratory sample identification | Linked DIME Sample ID | ||
The fabricator/manufacturer/facility name | Scougal Rubber | Transportation Laboratory (TL) Number | |
Inspector Lot Number from the Transportation Laboratory (TL) Form | Structure unique identifier | Not set | |
Structure name | Not set |
Material Information
Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 17375-1 |
---|---|---|---|
Material/Compound/Elastomer ID | NA | Samples Representing | 29 |
Description (size) | 2"x12"x12" | Comments | Unknown |
Description (Number of Shims) | 4 | Type of Bearing Pad | Steel |
Description (Thickness of Shims) | 14 gage | Manufacturer(s) | Scougal Rubber |
Batch Number | NA |
Test Details
DIME Sample ID: 2019-03-07-4
DIME Test ID: 2019-03-07-4-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2019-03-27
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steve
Date of test: 03/11/2019
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.068 in
Sample 1 Tear Strength: 205.9 lbf / in
Sample 2 Median Thickness: 0.068 in
Sample 2 Tear Strength: 191.2 lbf / in
Sample 3 Median Thickness: 0.065 in
Sample 3 Tear Strength: 200 lbf / in
UTM: no data
Median of the Tear Strength Values: 200 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 3/20/2019 ✔