Summary for Test 2016-07-06-12-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 210812
DEA: 041A3404
EFIS: 0412000162
DIST-CO-RTE-PM04-SCL-9-3.6,11.4
Award Date01/19/2016
Closeout Date12/21/2017
Work DescriptionREPLACE EXISTING BRIDGE RAILING.
Location DescriptionIN SANTA CLARA COUNTY IN SARATOGA AND LOS GATOS AT WEST BRANCHSARATOGA CREEK BRIDGE AND ATSARATOGA AVENUE SEPARATION
QA Service Level1 (Verified on 09/18/2015)

Sample Information

Sample Taken Date07/06/2016 Sample Unique Key12
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing07/20/2016
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes1 From where was the sample collectedSource
First name of sampler or witnessed byGreg Last name of sampler or witnessed byThompson
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameDynatect Transportation Laboratory (TL) NumberC836002
Inspector Lot Number from the Transportation Laboratory (TL) FormB907116 Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)051116
Material/Compound/Elastomer IDNA Samples Representing43
Description (size)1in x 4in x 6in CommentsUnknown
Description (Number of Shims)2 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Dynatect
Batch NumberNA

Test Details

DIME Sample ID: 2016-07-06-12
DIME Test ID: 2016-07-06-12-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2016-08-01

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 07/26/2016
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.075 in
Sample 1 Tear Strength: 253.3 lbf / in
Sample 2 Median Thickness: 0.068 in
Sample 2 Tear Strength: 294.1 lbf / in
Sample 3 Median Thickness: 0.066 in
Sample 3 Tear Strength: 287.9 lbf / in
UTM: no data
Median of the Tear Strength Values: 287.9 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 8/1/2016