Summary for Test 2019-12-26-2-3
Test performed: ASTM D624-00-re12Project Information
Project Identifiers | Project ID: 210837 DEA: 080J0804 EFIS: 0800000283 COOP: 081625 |
---|---|
DIST-CO-RTE-PM | 08-RIV-15-34.7/51.6 |
Award Date | 04/17/2017 |
Closeout Date | Not set |
Work Description | (Alternative Delivery) DESIGN-BUILD OF THE INTERSTATE 15 EXPRESS LANES PROJECT |
Location Description | Riverside County and SBD-15-0.0/1.3 |
QA Service Level | 1 (Verified on 05/08/2017) |
Sample Information
Sample Taken Date | 12/26/2019 | Sample Unique Key | 2 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 01/06/2020 |
Sample type | Quality Assurance | A brief description of the sample | elastomeric bearing pad |
The quantity of what the sample constitutes | 9 | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | Howard | Last name of sampler or witnessed by | Sternberg |
Title of sampler | Telephone number of sampler | ||
Laboratory sample identification | Linked DIME Sample ID | ||
The fabricator/manufacturer/facility name | Scougal Rubber | Transportation Laboratory (TL) Number | |
Inspector Lot Number from the Transportation Laboratory (TL) Form | Structure unique identifier | ||
Structure name |
Material Information
Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 18440-1 |
---|---|---|---|
Material/Compound/Elastomer ID | na | Samples Representing | 9 |
Description (size) | 3x14x18 | Comments | Unknown |
Description (Number of Shims) | 6 | Type of Bearing Pad | Steel |
Description (Thickness of Shims) | 14 gage | Manufacturer(s) | Scougal Rubber |
Batch Number | na |
Test Details
DIME Sample ID: 2019-12-26-2
DIME Test ID: 2019-12-26-2-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2020-01-14
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: randelin
Date of test: 01/08/2020
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.08
Sample 1 Tear Strength: 217.6
Sample 2 Median Thickness: 0.081
Sample 2 Tear Strength: 225.1
Sample 3 Median Thickness: 0.079
Sample 3 Tear Strength: 203.8
UTM: 2kip
Median of the Tear Strength Values: 217.6 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point FileTest graph for Sample 2
Source: Bluehill Data Point File
Test graph for Sample 3
Source: Bluehill Data Point File
Test graph for Sample 1
Test was verified on 1/14/2020 ✔