Summary for Test 2019-06-17-11-4

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 213569
DEA: 024F2104
EFIS: 0212000072
DIST-CO-RTE-PM02-MOD-299-0.5/1.0
Award Date12/20/2018
Closeout Date11/15/2021
Work DescriptionButte and Ash Creek Bridge Replacement
Location DescriptionConstruction of Butte Creek Bridge and Ash Creek Bridge on Route 299 at Adin
QA Service Level1 (Verified on 06/26/2019)

Sample Information

Sample Taken Date06/17/2019 Sample Unique Key11
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing06/19/2019
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes2 From where was the sample collectedManufacturer
First name of sampler or witnessed byPete Last name of sampler or witnessed byEtcheverry
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameScougal Rubber Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifier
Structure name

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)17865-2
Material/Compound/Elastomer IDna Samples Representing62
Description (size)2" x 12" x 24" CommentsUnknown
Description (Number of Shims)4 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch Numberna

Test Details

DIME Sample ID: 2019-06-17-11
DIME Test ID: 2019-06-17-11-4
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2019-06-26

Test Results


Number of specimens tested: 5
Input Type: Measured
Tester's full name: Steve
Date of test: 06/21/2019
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.07 in
Sample 1 Tear Strength: 185.7 lbf / in
Sample 2 Median Thickness: 0.069 in
Sample 2 Tear Strength: 173.9 lbf / in
Sample 3 Median Thickness: 0.069 in
Sample 3 Tear Strength: 188.4 lbf / in
Sample 4 Median Thickness: 0.067 in
Sample 4 Tear Strength: 179.1 lbf / in
Sample 5 Median Thickness: 0.068 in
Sample 5 Tear Strength: 176.5 lbf / in
UTM: no data
Median of the Tear Strength Values: 179.1 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Source: Partner Data Point File
Test graph for Sample 4

Source: Partner Data Point File
Test graph for Sample 5

Test was verified on 6/26/2019