Summary for Test 2020-10-22-2-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 77777
DEA: CHEM-STOCK
EFIS: CHEM-STOCK
DIST-CO-RTE-PM59---
Award DateNot set
Closeout DateNot set
Work DescriptionSpecial project for Chem Lab stock material. Object Code: 1025. J2 DEA: 912680.
Location DescriptionNot set
QA Service LevelNOT VERIFIED

Sample Information

Sample Taken Date10/22/2020 Sample Unique Key2
Date that the sample was received by the laboratory/organization performing the testing10/23/2020 Sample typeQuality Assurance
A brief description of the sample3/8" x 48" Neoprene bearing pad The quantity of what the sample constitutes117 Lft
From where was the sample collectedDistributor First name of sampler or witnessed byKevin
Last name of sampler or witnessed byCarpenter Title of samplerQA Consultant
Telephone number of sampler415-608-1742 Laboratory sample identification
Linked DIME Sample ID The fabricator/manufacturer/facility nameCal Neva Supply
Transportation Laboratory (TL) Number Inspector Lot Number from the Transportation Laboratory (TL) FormB24-050-20
Structure unique identifier Structure name
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)020620
Material/Compound/Elastomer ID0012270880 Samples Representing117 Lft
Description (size).375X48" Comments
Description (Number of Shims)0 Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)020620
Batch Number8168

Test Details

DIME Sample ID: 2020-10-22-2
DIME Test ID: 2020-10-22-2-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2020-10-29

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: spaine
Date of test: 10/26/2020
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.08
Sample 1 Tear Strength: 249.2
Sample 2 Median Thickness: 0.08
Sample 2 Tear Strength: 229.6
Sample 3 Median Thickness: 0.081
Sample 3 Tear Strength: 243.6
UTM: 2kip
Median of the Tear Strength Values: 243.6 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point File
Test graph for Sample 2

Source: Bluehill Data Point File
Test graph for Sample 1

Source: Bluehill Data Point File
Test graph for Sample 3

Test was verified on 10/29/2020 ✔