Summary for Test 2020-01-17-2-3
Test performed: ASTM D624-00-re12Project Information
| Project Identifiers | Project ID: 214392 DEA: 100H4804 EFIS: 1012000193 |
|---|---|
| DIST-CO-RTE-PM | 10-STA-108-33.1/33.4 |
| Award Date | 11/13/2019 |
| Closeout Date | 03/08/2021 |
| Work Description | COLD PLANE AC SURFACING, HMA (TYPE A) RESURFACING, AND BRIDGE REPAIR. |
| Location Description | STANISLAUS COUNTY IN RIVERBANK FROM 0.1 MILE WEST OF EIGHTH STREET TO 0.1 MILE EAST OF CLAUS ROAD |
| QA Service Level | 1 (Verified on 09/13/2019) |
Sample Information
| Sample Taken Date | 01/17/2020 | Sample Unique Key | 2 |
|---|---|---|---|
| Date that the sample was received by the laboratory/organization performing the testing | 01/21/2020 | Sample type | Quality Assurance |
| A brief description of the sample | elastomeric bearing pad | The quantity of what the sample constitutes | 1 |
| From where was the sample collected | Manufacturer | First name of sampler or witnessed by | Howard |
| Last name of sampler or witnessed by | Sternberg | Title of sampler | |
| Telephone number of sampler | Laboratory sample identification | ||
| Linked DIME Sample ID | The fabricator/manufacturer/facility name | Scougal Rubber | |
| Transportation Laboratory (TL) Number | Inspector Lot Number from the Transportation Laboratory (TL) Form | ||
| Structure unique identifier | Structure name | ||
| Bid Item | Not set |
Material Information
| Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 18496-1 |
|---|---|---|---|
| Material/Compound/Elastomer ID | na | Samples Representing | 7 |
| Description (size) | 3x10x12 | Comments | Unknown |
| Description (Number of Shims) | 6 | Type of Bearing Pad | Steel |
| Description (Thickness of Shims) | 14 gage | Manufacturer(s) | Scougal Rubber |
| Batch Number | na |
Test Details
DIME Sample ID: 2020-01-17-2
DIME Test ID: 2020-01-17-2-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2020-01-28
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: randelin
Date of test: 01/23/2020
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.08
Sample 1 Tear Strength: 208.2
Sample 2 Median Thickness: 0.076
Sample 2 Tear Strength: 209.5
Sample 3 Median Thickness: 0.076
Sample 3 Tear Strength: 203.5
UTM: 2kip
Median of the Tear Strength Values: 208.2 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point FileTest graph for Sample 1
Source: Bluehill Data Point File
Test graph for Sample 3
Source: Bluehill Data Point File
Test graph for Sample 2
Test was verified on 1/28/2020 ✔