Summary for Test 2026-07-13-34-3

Test performed: ASTM D624-00r20

Project Information

Project IdentifiersProject ID: 1001971
DEA: 010Q4104
EFIS: 0125000175
DIST-CO-RTE-PM01-HUM-101-35.75/35.75
Award DateNot set
Closeout DateNot set
Work DescriptionNot set
Location DescriptionNot set
QA Service Level1 (Verified on 02/26/2026)

Sample Information

Sample Taken Date07/13/2026 Sample Unique Key34
Will the laboratory/organization for which you are a member perform testing on this material sample?No Date that the sample was received by the laboratory/organization performing the testing07/20/2026
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutesX From where was the sample collectedManufacturer
First name of sampler or witnessed byKrishnamoorthy Last name of sampler or witnessed byPalaniappan
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameBridge Rubber Bearing Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifier
Structure name Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)2527-4
Material/Compound/Elastomer IDNA Samples Representing7
Description (size)1.73" x 14" x 16" Comments
Description (Number of Shims)3 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Bridge Rubber Bearing
Batch Number158253

Test Details

DIME Sample ID: 2026-07-13-34
DIME Test ID: 2026-07-13-34-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2026-08-06

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Andrew Auvinen
Date of test: 08/06/2026
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.075 in
Sample 1 Tear Strength: 235 lb/in
Sample 2 Median Thickness: 0.074 in
Sample 2 Tear Strength: 256 lb/in
Sample 3 Median Thickness: 0.074 in
Sample 3 Tear Strength: 212 lb/in
UTM: NA
Median of the Tear Strength Values: 235 lb/in
General comments (publicly viewable) (Max 1000 characters):

Test was verified on 8/6/2026