Summary for Test 2026-06-22-73-5
Test performed: ASTM D624-00r20Project Information
| Project Identifiers | Project ID: 1002077 DEA: 033H5904 EFIS: 0318000017 |
|---|---|
| DIST-CO-RTE-PM | 03-PLA-80-R26.3/R55.2 |
| Award Date | 01/08/2026 |
| Closeout Date | Not set |
| Work Description | Not set |
| Location Description | Not set |
| QA Service Level | 1 (Verified on 04/07/2026) |
Sample Information
| Sample Taken Date | 06/22/2026 | Sample Unique Key | 73 |
|---|---|---|---|
| Date that the sample was received by the laboratory/organization performing the testing | 07/07/2026 | Sample type | Quality Assurance |
| A brief description of the sample | Bearing Pad Plain | The quantity of what the sample constitutes | 178 |
| From where was the sample collected | Manufacturer | First name of sampler or witnessed by | Mario |
| Last name of sampler or witnessed by | Rodriguez | Title of sampler | |
| Telephone number of sampler | Laboratory sample identification | ||
| Linked DIME Sample ID | The fabricator/manufacturer/facility name | Scougal Rubber | |
| Transportation Laboratory (TL) Number | Inspector Lot Number from the Transportation Laboratory (TL) Form | ||
| Structure unique identifier | Structure name | ||
| Bid Item | Not set |
Material Information
| Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 27837-4 |
|---|---|---|---|
| Material/Compound/Elastomer ID | NA | Samples Representing | 178 |
| Description (size) | 1" X 8" X 24" | Comments | |
| Description (Number of Shims) | 0 | Type of Bearing Pad | Plain |
| Description (Thickness of Shims) | NA | Manufacturer(s) | Scougal Rubber |
| Batch Number | NA |
Test Details
DIME Sample ID: 2026-06-22-73
DIME Test ID: 2026-06-22-73-5
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2026-08-06
Test Results
Number of specimens tested: 5
Input Type: Measured
Tester's full name: Andrew Auvinen
Date of test: 08/06/2026
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.076 in
Sample 1 Tear Strength: 158 lb/in
Sample 2 Median Thickness: 0.076 in
Sample 2 Tear Strength: 202 lb/in
Sample 3 Median Thickness: 0.062 in
Sample 3 Tear Strength: 193 lb/in
Sample 4 Median Thickness: 0.082 in
Sample 4 Tear Strength: 175 lb/in
Sample 5 Median Thickness: 0.075 in
Sample 5 Tear Strength: 202 lb/in
UTM: NA
Median of the Tear Strength Values: 193 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test was verified on 8/6/2026 ✔