Summary for Test 2026-06-19-33-3

Test performed: ASTM D624-00r20

Project Information

Project IdentifiersProject ID: 1001640
DEA: 010N2904
EFIS: 0123000202
DIST-CO-RTE-PM01-DN-197,199-Var
Award DateNot set
Closeout DateNot set
Work DescriptionREPLACE BRIDGE, EXCAVATION, AND RETAINING WALLS.
Location DescriptionDEL NORTE COUNTY AT VARIOUS LOCATIONS
QA Service Level1 (Verified on 09/22/2025)

Sample Information

Sample Taken Date06/19/2026 Sample Unique Key33
Date that the sample was received by the laboratory/organization performing the testing06/26/2026 Sample typeQuality Assurance
A brief description of the sampleVersiflex Elastomeric Pad The quantity of what the sample constitutes16
From where was the sample collectedManufacturer First name of sampler or witnessed byJustin
Last name of sampler or witnessed byCrawford Title of sampler
Telephone number of sampler Laboratory sample identification
Linked DIME Sample ID The fabricator/manufacturer/facility nameDS Brown
Transportation Laboratory (TL) Number Inspector Lot Number from the Transportation Laboratory (TL) Form
Structure unique identifier Structure name
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)1090477-1102-2A
Material/Compound/Elastomer IDna Samples Representing16
Description (size)18.5" x 15.75" x 1" Comments
Description (Number of Shims)NA Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)DS Brown
Batch Numberna

Test Details

DIME Sample ID: 2026-06-19-33
DIME Test ID: 2026-06-19-33-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2026-07-16

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steven Paine
Date of test: 07/16/2026
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.071 in
Sample 1 Tear Strength: 282 lb/in
Sample 2 Median Thickness: 0.076 in
Sample 2 Tear Strength: 286 lb/in
Sample 3 Median Thickness: 0.089 in
Sample 3 Tear Strength: 275 lb/in
UTM: NA
Median of the Tear Strength Values: 282 lb/in
General comments (publicly viewable) (Max 1000 characters):

Test was verified on 7/16/2026 ✔