Summary for Test 2018-04-09-4-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 212731
DEA: 07318004
EFIS: 0715000280
DIST-CO-RTE-PM07-LA-10-22.3/28.2
Award Date11/16/2017
Closeout Date06/16/2021
Work DescriptionTREAT BRIDGE DECK, CLOSURE POUR AND REPLACE JOINT SEALS.
Location DescriptionLOS ANGELES COUNTY AT VARIOUS LOCATIONS FROM FREMONT AVENUE UNDERCROSSING TO RIO HONDO62
QA Service Level1 (Verified on 03/21/2018)

Sample Information

Sample Taken Date04/09/2018 Sample Unique Key4
Date that the sample was received by the laboratory/organization performing the testing04/10/2018 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes1
From where was the sample collectedManufacturer First name of sampler or witnessed byPete
Last name of sampler or witnessed byEtcheverry Title of samplerUnknown
Telephone number of samplerUnknown Laboratory sample identificationUnknown
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility nameScougal Rubber
Transportation Laboratory (TL) NumberUnknown Inspector Lot Number from the Transportation Laboratory (TL) FormUnknown
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)16714-1
Material/Compound/Elastomer ID2 527 Samples Representing4
Description (size)2.5"x12"x24" CommentsUnknown
Description (Number of Shims)5 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch Number0

Test Details

DIME Sample ID: 2018-04-09-4
DIME Test ID: 2018-04-09-4-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2018-04-20

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Randy
Date of test: 04/11/2018
Humidity: 50 %
Temperature: no data
Sample 1 Median Thickness: 0.079 in
Sample 1 Tear Strength: 217.7 lbf / in
Sample 2 Median Thickness: 0.079 in
Sample 2 Tear Strength: 219 lbf / in
Sample 3 Median Thickness: 0.081 in
Sample 3 Tear Strength: 196.3 lbf / in
UTM: no data
Median of the Tear Strength Values: 217.7 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 4/13/2018 ✔