Summary for Test 2018-03-13-9-2

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 212748
DEA: 081F2704
EFIS: 0814000195
DIST-CO-RTE-PM08-SBD-210-R29.3/R33.0
Award Date12/04/2017
Closeout Date06/23/2021
Work DescriptionTREAT DECK, REPLACE JOINT SEALS AND ELASTOMERIC BEARING PADS
Location DescriptionSAN BERNARDINO COUNTY IN REDLANDS AND HIGHLAND AT VARIOUS LOCATIONS FROM BASELINE ROAD TO ROUTE 210/10 SEPARATION
QA Service Level1 (Verified on 01/05/2018)

Sample Information

Sample Taken Date03/13/2018 Sample Unique Key9
Date that the sample was received by the laboratory/organization performing the testing03/15/2018 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes1
From where was the sample collectedManufacturer First name of sampler or witnessed byPete
Last name of sampler or witnessed byEtcheverry Title of samplerQuality Manager
Telephone number of samplerUnknown Laboratory sample identificationUnknown
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility nameScougal Rubber
Transportation Laboratory (TL) NumberUnknown Inspector Lot Number from the Transportation Laboratory (TL) FormUnknown
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)16487-1
Material/Compound/Elastomer IDUnknown Samples Representing7
Description (size)3.5"x20"x22" CommentsUnknown
Description (Number of Shims)7 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch NumberUnknown

Test Details

DIME Sample ID: 2018-03-13-9
DIME Test ID: 2018-03-13-9-2
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2018-04-02

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Randy
Date of test: 03/19/2018
Humidity: 50 %
Temperature: 70 F
Sample 1 Median Thickness: 0.074 in
Sample 1 Tear Strength: 216.2 lbf / in
Sample 2 Median Thickness: 0.069 in
Sample 2 Tear Strength: 231.9 lbf / in
Sample 3 Median Thickness: 0.069 in
Sample 3 Tear Strength: 202.9 lbf / in
UTM: no data
Median of the Tear Strength Values: 216.2 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 3/26/2018 ✔