Summary for Test 2026-03-17-34-7
Test performed: ASTM D624-00r20Project Information
| Project Identifiers | Project ID: 993798 DEA: 09366804 EFIS: 0916000021 |
|---|---|
| DIST-CO-RTE-PM | 09-INY-395-117.3/117.9 |
| Award Date | 04/03/2025 |
| Closeout Date | Not set |
| Work Description | MEADOW FARMS ADA |
| Location Description | INYO COUNTY NEAR BISHOP FROM 0.1 MILE EAST OF SEE VEE LANE TO BARLOW LANE |
| QA Service Level | 1 (Verified on 08/14/2023) |
Sample Information
| Sample Taken Date | 03/17/2026 | Sample Unique Key | 34 |
|---|---|---|---|
| Date that the sample was received by the laboratory/organization performing the testing | 03/23/2026 | Sample type | Quality Assurance |
| A brief description of the sample | 1"x4"x6" Elastomeric Bearing Pad | The quantity of what the sample constitutes | 100 |
| From where was the sample collected | Manufacturer | First name of sampler or witnessed by | Mario |
| Last name of sampler or witnessed by | Rodriguez | Title of sampler | |
| Telephone number of sampler | Laboratory sample identification | ||
| Linked DIME Sample ID | The fabricator/manufacturer/facility name | Scougal Rubber | |
| Transportation Laboratory (TL) Number | Inspector Lot Number from the Transportation Laboratory (TL) Form | ||
| Structure unique identifier | Structure name | ||
| Bid Item | Not set |
Material Information
| Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 27569-1 |
|---|---|---|---|
| Material/Compound/Elastomer ID | 2527 | Samples Representing | 100 |
| Description (size) | 1X4X6 | Comments | |
| Description (Number of Shims) | NA | Type of Bearing Pad | Plain |
| Description (Thickness of Shims) | NA | Manufacturer(s) | Scougal |
| Batch Number | 27569-1 |
Test Details
DIME Sample ID: 2026-03-17-34
DIME Test ID: 2026-03-17-34-7
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2026-04-20
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steven Paine
Date of test: 04/20/2026
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.075 in
Sample 1 Tear Strength: 194 lb/in
Sample 2 Median Thickness: 0.082 in
Sample 2 Tear Strength: 180 lb/in
Sample 3 Median Thickness: 0.077 in
Sample 3 Tear Strength: 185 lb/in
UTM: NA
Median of the Tear Strength Values: 185 lb/in
General comments (publicly viewable) (Max 1000 characters): sample 2
Test was verified on 4/20/2026 ✔