Summary for Test 2018-01-29-6-4

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 212795
DEA: 05937704
EFIS: 0514901244
Permit Numbers: 05176UB0132
DIST-CO-RTE-PM05-MON-68-4.04
Award Date09/06/2017
Closeout Date05/24/2019
Work DescriptionInstall a water pipeline bridge including a 36 inch diameter steel casing
Location DescriptionCounty of Monterey
QA Service Level1 (Verified on 09/25/2017)

Sample Information

Sample Taken Date01/29/2018 Sample Unique Key6
Date that the sample was received by the laboratory/organization performing the testing02/02/2018 Sample typeQuality Assurance
A brief description of the sampleElastomeric Bearing Pad The quantity of what the sample constitutes1
From where was the sample collectedManufacturer First name of sampler or witnessed byChristy
Last name of sampler or witnessed byStockton Title of samplerUnknown
Telephone number of samplerUnknown Laboratory sample identification16202-1, 16202-2
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility nameScougal Rubber
Transportation Laboratory (TL) NumberUnknown Inspector Lot Number from the Transportation Laboratory (TL) FormUnknown
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)16202-1, 16202-2
Material/Compound/Elastomer ID2 527 Samples Representing16202 1
Description (size)3 x 10 x 14 CommentsUnknown
Description (Number of Shims)6 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch NumberUnknown

Test Details

DIME Sample ID: 2018-01-29-6
DIME Test ID: 2018-01-29-6-4
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2018-02-28

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Fred
Date of test: 02/08/2018
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.075 in
Sample 1 Tear Strength: 200 lbf / in
Sample 2 Median Thickness: 0.08 in
Sample 2 Tear Strength: 200 lbf / in
Sample 3 Median Thickness: 0.088 in
Sample 3 Tear Strength: 215.9 lbf / in
UTM: no data
Median of the Tear Strength Values: 200 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 2/21/2018 ✔