Summary for Test 2025-12-18-33-3

Test performed: ASTM D624-00r20

Project Information

Project IdentifiersProject ID: 88888
DEA: SMTL-STOCK
EFIS: SMTL-STOCK
DIST-CO-RTE-PM59---
Award DateNot set
Closeout DateNot set
Work DescriptionSpecial project for SMTL stock material. Object Code: 1025. J2 DEA: 912680.
Location DescriptionNot set
QA Service LevelNOT VERIFIED

Sample Information

Sample Taken Date12/18/2025 Sample Unique Key33
Will the laboratory/organization for which you are a member perform testing on this material sample?No Date that the sample was received by the laboratory/organization performing the testing12/22/2025
Sample typeQuality Assurance A brief description of the sample1/4" X 48" 55 DURO BEARING PAD
The quantity of what the sample constitutes1/4" X 48" 55 DURO BEARING PAD From where was the sample collectedSupplier
First name of sampler or witnessed byNIKHIL Last name of sampler or witnessed byMOON
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameCal Neva Supply Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifier
Structure name Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)LOT# 1390590
Material/Compound/Elastomer IDLOT 1390590 Samples RepresentingCALNEVA
Description (size)1 FT X 1 FT Comments
Description (Number of Shims)NA Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)CALNEVA
Batch NumberLOT 1390590

Test Details

DIME Sample ID: 2025-12-18-33
DIME Test ID: 2025-12-18-33-3
Testing Lab: Phoenix National Lab
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2026-01-27

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Andrew Auvinen
Date of test: 01/26/2026
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.076 in
Sample 1 Tear Strength: 181 lb/in
Sample 2 Median Thickness: 0.082 in
Sample 2 Tear Strength: 183 lb/in
Sample 3 Median Thickness: 0.077 in
Sample 3 Tear Strength: 188 lb/in
UTM: NA
Median of the Tear Strength Values: 183 lb/in
General comments (publicly viewable) (Max 1000 characters):

Test was verified on 1/27/2026