Summary for Test 2025-01-16-35-3

Test performed: ASTM D624-00r20

Project Information

Project IdentifiersProject ID: 1000272
DEA: 100V4804
EFIS: 1013000264
DIST-CO-RTE-PM10-CAL-26-21.8/30.3
Award Date09/09/2024
Closeout Date08/20/2026
Work DescriptionSLOPE STABILIZATION AND CONSTRUCT RETAINING WALL.
Location DescriptionCALAVERAS COUNTY NEAR MOKELUMNE HILL AT VARIOUS LOCATIONS FROM 3.6 MILES EAST OF ROUTE 49 TO 0.9 MILE WEST OF WOODHOUSE MINE ROAD
QA Service Level1 (Verified on 04/15/2024)

Sample Information

Sample Taken Date01/16/2025 Sample Unique Key35
Date that the sample was received by the laboratory/organization performing the testing01/22/2025 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes179
From where was the sample collectedManufacturer First name of sampler or witnessed byKrishnamoorthy
Last name of sampler or witnessed byPalaniappan Title of sampler
Telephone number of sampler Laboratory sample identification
Linked DIME Sample ID The fabricator/manufacturer/facility nameBridge Rubber Bearing
Transportation Laboratory (TL) Number Inspector Lot Number from the Transportation Laboratory (TL) Form
Structure unique identifier Structure name
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)2527-1
Material/Compound/Elastomer IDNA Samples Representing179
Description (size)1" x 8" x 12" Comments
Description (Number of Shims)0 Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)Bridge Rubber Bearing
Batch Number144285

Test Details

DIME Sample ID: 2025-01-16-35
DIME Test ID: 2025-01-16-35-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2025-02-13

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steven Paine
Date of test: 02/13/2025
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.091 in
Sample 1 Tear Strength: 231 lb/in
Sample 2 Median Thickness: 0.099 in
Sample 2 Tear Strength: 236 lb/in
Sample 3 Median Thickness: 0.091 in
Sample 3 Tear Strength: 237 lb/in
UTM: NA
Median of the Tear Strength Values: 236 lb/in
General comments (publicly viewable) (Max 1000 characters):

Test was verified on 2/13/2025 ✔