Summary for Test 2024-06-13-129-3
Test performed: ASTM D624-00r20Project Information
| Project Identifiers | Project ID: 88888 DEA: SMTL-STOCK EFIS: SMTL-STOCK |
|---|---|
| DIST-CO-RTE-PM | 59--- |
| Award Date | Not set |
| Closeout Date | Not set |
| Work Description | Special project for SMTL stock material. Object Code: 1025. J2 DEA: 912680. |
| Location Description | Not set |
| QA Service Level | NOT VERIFIED |
Sample Information
| Sample Taken Date | 06/13/2024 | Sample Unique Key | 129 |
|---|---|---|---|
| Date that the sample was received by the laboratory/organization performing the testing | 12/02/2024 | Sample type | Quality Assurance |
| A brief description of the sample | Bearing Pad | The quantity of what the sample constitutes | 3 |
| From where was the sample collected | Manufacturer | First name of sampler or witnessed by | Rob |
| Last name of sampler or witnessed by | Anderson | Title of sampler | |
| Telephone number of sampler | Laboratory sample identification | ||
| Linked DIME Sample ID | The fabricator/manufacturer/facility name | Scougal Rubber | |
| Transportation Laboratory (TL) Number | Inspector Lot Number from the Transportation Laboratory (TL) Form | ||
| Structure unique identifier | Structure name | ||
| Bid Item | Not set |
Material Information
| Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | NA |
|---|---|---|---|
| Material/Compound/Elastomer ID | 33312 | Samples Representing | 3 |
| Description (size) | NA | Comments | |
| Description (Number of Shims) | 0 | Type of Bearing Pad | Plain |
| Description (Thickness of Shims) | NA | Manufacturer(s) | Scougal Rubber |
| Batch Number | NA |
Test Details
DIME Sample ID: 2024-06-13-129
DIME Test ID: 2024-06-13-129-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2025-01-22
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Steven Paine
Date of test: 01/22/2025
Humidity: 0 %
Temperature: 0 f
Sample 1 Median Thickness: 0.086 in
Sample 1 Tear Strength: 227 lb/in
Sample 2 Median Thickness: 0.074 in
Sample 2 Tear Strength: 223 lb/in
Sample 3 Median Thickness: 0.08 in
Sample 3 Tear Strength: 229 lb/in
UTM: NA
Median of the Tear Strength Values: 227 lb/in