Summary for Test 2017-07-31-4-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 211260
DEA: 072159U4
EFIS: 0715000160
DIST-CO-RTE-PM07-LA,ORA-5-0.0/1.5, 44.3/44.4
Award Date05/27/2016
Closeout Date08/01/2023
Work DescriptionCONSTRUCT HOV LANES AND MIX FLOW LANES.
Location DescriptionLOS ANGELES AND ORANGE COUNTIES IN BUENA PARK, LA MIRADA, CERRITOS AND SANTA FE SPRINGS FROM ARTESIA BOULEVARD UNDERCROSSING TO NORTH FORK COYOTE CREEK
QA Service Level1 (Verified on 03/16/2016)

Sample Information

Sample Taken Date07/31/2017 Sample Unique Key4
Date that the sample was received by the laboratory/organization performing the testing08/11/2017 Sample typeQuality Assurance
A brief description of the sample.75x8x12 Bearing Pad The quantity of what the sample constitutes2
From where was the sample collectedManufacturer First name of sampler or witnessed byScott
Last name of sampler or witnessed byLeavitt Title of samplerQA Inspector
Telephone number of sampler5105900116 Laboratory sample identificationUnknown
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility nameScougal Rubber
Transportation Laboratory (TL) NumberUnknown Inspector Lot Number from the Transportation Laboratory (TL) FormS28-201-17
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)16066-1
Material/Compound/Elastomer IDCP2527V55DURO Samples Representing2
Description (size).75x8x12 CommentsUnknown
Description (Number of Shims)Plain Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)Scougal Rubber
Batch NumberUnknown

Test Details

DIME Sample ID: 2017-07-31-4
DIME Test ID: 2017-07-31-4-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-08-23

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 08/15/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.061 in
Sample 1 Tear Strength: 278.7 lbf / in
Sample 2 Median Thickness: 0.083 in
Sample 2 Tear Strength: 241 lbf / in
Sample 3 Median Thickness: 0.06 in
Sample 3 Tear Strength: 233.3 lbf / in
UTM: no data
Median of the Tear Strength Values: 241 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 8/16/2017