Summary for Test 2024-09-24-21-5

Test performed: AASHTO T308-10

Project Information

Project IdentifiersProject ID: 1000165
DEA: 09392504
EFIS: 0923000029
DIST-CO-RTE-PM09-INY-395-R17.2/25.8
Award Date06/26/2024
Closeout Date12/02/2024
Work DescriptionHOT MIX ASPHALT (TYPE A), SHOULDER BACKING, & STRIPING.
Location DescriptionINYO COUNTY ABOUT 9 MILES SOUTH OF OLANCHA FROM 0.8 MILE SOUTH OF SYKES ROAD TO 0.3 MILE NORTH OF HAIWEE CANYON ROAD
QA Service Level1 (Verified on 03/18/2024)

Sample Information

Sample Taken Date09/24/2024 Sample Unique Key21
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing09/24/2024
Sample typeQuality Assurance A brief description of the sampleHMA37
The quantity of what the sample constitutes24-28K Air Void, 20-30K Hammy From where was the sample collectedJob Site
First name of sampler or witnessed byJerid Last name of sampler or witnessed byKupelian
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameGranite Construction Arvin Plant Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifier
Structure name

Material Information

Material TypeHot Mix Asphalt HMA TypeType A HMA
HMA Grading1/2 inch Lot number1
Sublot number37 HMA Mix Number

Test Details

DIME Sample ID: 2024-09-24-21
DIME Test ID: 2024-09-24-21-5
Testing Lab: CT D09 - Bishop Field Laboratory
Test Method: AASHTO T308-10: Standard Method of Test for Determining the Asphalt Binder Content of Hot Mix Asphalt (HMA) by the Ignition Method (Method A) (Asphalt Binder Content)
Test Release Date: 2024-09-26

Test Results


What temperature unit is used?: Celsius
Input Type: Measured
Tester's full name: Derek Carrington
Date of test: 09/24/2024
Test procedure used?: Method A
Mass of the specimen basket assembly: 4256.2 g
Mass of the specimen and specimen basket assembly prior to ignition: 6004.7 g
Mass of HMA Sample prior to ignition: 1748.5 g
Mass Loss: 94.4 g
Mass of aggregate remaining after ignition: 1654.1 g
Correction Factor (Percent by mass of HMA Specimen): 0.35 %
Moisture Content: 0 %
Temperature Compensation Factor: 0 %
Test Temperature: 538 C
Corrected Asphalt Binder Content: 5.05 %
General comments (publicly viewable) (Max 1000 characters): HMA-37