Summary for Test 2024-09-13-34-1
Test performed: AASHTO T308-10Project Information
| Project Identifiers | Project ID: 994947 DEA: 112T3644 EFIS: 1121000108 |
|---|---|
| DIST-CO-RTE-PM | 11-SD-56-0.3/3.0 |
| Award Date | 10/17/2023 |
| Closeout Date | Not set |
| Work Description | CONSTRUCT JPCP, HMA, RHMA-G, SIGNS, BARRIERS, LANDSCAPE, & ELECTRICAL. |
| Location Description | SAN DIEGO COUNTY IN SAN DIEGO FROM EL CAMINO REAL UNDERCROSSING TO 0.3 MILE WEST OF CARMEL VALLEY ROAD OVERCROSSING |
| QA Service Level | 1 (Verified on 01/22/2024) |
Sample Information
| Sample Taken Date | 09/13/2024 | Sample Unique Key | 34 |
|---|---|---|---|
| Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 09/17/2024 |
| Sample type | Quality Assurance | A brief description of the sample | Milestone |
| The quantity of what the sample constitutes | 36 boxes | From where was the sample collected | Source |
| First name of sampler or witnessed by | Derrick | Last name of sampler or witnessed by | McCovy |
| Title of sampler | Telephone number of sampler | 6192463546 | |
| Laboratory sample identification | 09018-MS | Linked DIME Sample ID | |
| The fabricator/manufacturer/facility name | Martin Marietta | Transportation Laboratory (TL) Number | |
| Inspector Lot Number from the Transportation Laboratory (TL) Form | Structure unique identifier | ||
| Structure name | Bid Item | Not set |
Material Information
| Material Type | Hot Mix Asphalt | HMA Type | Type A HMA |
|---|---|---|---|
| HMA Grading | 3/4 inch | Lot number | |
| Sublot number | HMA Mix Number | 23417005SR MM | |
| Binder content (%) | Not set | Virgin binder PG | Not set |
| Design binder PG | Not set | Binder Supplier | Not set |
| RAP content (%) | Not set | WMA Additives | Not set |
| Antistrip type | Not set |
Test Details
DIME Sample ID: 2024-09-13-34
DIME Test ID: 2024-09-13-34-1
Testing Lab: CT D11 - District 11 Materials Laboratory
Test Method: AASHTO T308-10: Standard Method of Test for Determining the Asphalt Binder Content of Hot Mix Asphalt (HMA) by the Ignition Method (Method A) (Asphalt Binder Content)
Test Release Date: 2024-09-27
Test Results
What temperature unit is used?: Celsius
Input Type: Measured
Tester's full name: Shawn Rivers
Date of test: 09/24/2024
Test procedure used?: Method A
Mass of the specimen basket assembly: 4014.6 g
Mass of the specimen and specimen basket assembly prior to ignition: 6041.5 g
Mass of HMA Sample prior to ignition: 2026.9 g
Mass Loss: 113.4 g
Mass of aggregate remaining after ignition: 1913.5 g
Correction Factor (Percent by mass of HMA Specimen): 0.44 %
Moisture Content: 0.00 %
Temperature Compensation Factor: 0.00 %
Test Temperature: 538 C
Corrected Asphalt Binder Content: 5.15 %
General comments (publicly viewable) (Max 1000 characters):
Test was verified on 9/27/2024 ✔