Summary for Test 2017-07-21-4-3
Test performed: ASTM D624-00-re12Project Information
| Project Identifiers | Project ID: 212222 DEA: 033H1004 |
|---|---|
| DIST-CO-RTE-PM | 03-ED-50-37.6, 37.60 |
| Award Date | 03/16/2017 |
| Closeout Date | 01/09/2019 |
| Work Description | Construct Soldier Pile Wall |
| Location Description | Not set |
| QA Service Level | 1 (Verified on 06/19/2017) |
Sample Information
| Sample Taken Date | 07/21/2017 | Sample Unique Key | 4 |
|---|---|---|---|
| Date that the sample was received by the laboratory/organization performing the testing | 07/25/2017 | Sample type | Department Acceptance |
| A brief description of the sample | 1x8x12 Steel Reinforced | The quantity of what the sample constitutes | 63 |
| From where was the sample collected | Manufacturer | First name of sampler or witnessed by | Kevin |
| Last name of sampler or witnessed by | Muser | Title of sampler | QA |
| Telephone number of sampler | 916-517-0532 | Laboratory sample identification | |
| Linked DIME Sample ID | The fabricator/manufacturer/facility name | Scougal Rubber | |
| Transportation Laboratory (TL) Number | Inspector Lot Number from the Transportation Laboratory (TL) Form | S19-408-17 | |
| Structure unique identifier | Not set | Structure name | Not set |
| Bid Item | Not set |
Material Information
| Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 179747V |
|---|---|---|---|
| Material/Compound/Elastomer ID | cp2527v55duroneogr3 | Samples Representing | 63 |
| Description (size) | 1x8x12 | Comments | |
| Description (Number of Shims) | 2 | Type of Bearing Pad | Steel |
| Description (Thickness of Shims) | 14 gage | Manufacturer(s) | Scougal Rubber |
| Batch Number | 16005 |
Test Details
DIME Sample ID: 2017-07-21-4
DIME Test ID: 2017-07-21-4-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-08-03
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 07/25/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.066 in
Sample 1 Tear Strength: 227.3 lbf / in
Sample 2 Median Thickness: 0.064 in
Sample 2 Tear Strength: 187.5 lbf / in
Sample 3 Median Thickness: 0.064 in
Sample 3 Tear Strength: 187.5 lbf / in
UTM: no data
Median of the Tear Strength Values: 187.5 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 7/27/2017 ✔