Summary for Test 2024-06-10-109-3

Test performed: ASTM D624-00r20

Project Information

Project IdentifiersProject ID: 994574
DEA: 050C7334
EFIS: 0518000116
DIST-CO-RTE-PM05-SCR-1-10.5/13.4
Award Date06/29/2023
Closeout DateNot set
Work DescriptionCONSTRUCT OVERCROSSING AND AUXILIARY LANE/ Replace Capitola Ave OC + RWs and SWs
Location DescriptionSANTA CRUZ COUNTY IN AND NEAR CITY OF CAPITOLA FROM STATE PARK DRIVE OVERCROSSING TO 0.2 MILE NORTH OF BAY AVENUE UNDERCROSSING
QA Service Level1 (Verified on 04/13/2023)

Sample Information

Sample Taken Date06/10/2024 Sample Unique Key109
Date that the sample was received by the laboratory/organization performing the testing07/01/2024 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes1
From where was the sample collectedManufacturer First name of sampler or witnessed byKrishnamoorthy
Last name of sampler or witnessed byPalaniappan Title of sampler
Telephone number of sampler Laboratory sample identification
Linked DIME Sample ID The fabricator/manufacturer/facility nameBridge Rubber Bearing
Transportation Laboratory (TL) Number Inspector Lot Number from the Transportation Laboratory (TL) Form
Structure unique identifier Structure name
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)2527-2
Material/Compound/Elastomer IDna Samples Representing27
Description (size)2.30" x 8" x 12" Comments
Description (Number of Shims)4 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Bridge Rubber Bearing
Batch Number138493

Test Details

DIME Sample ID: 2024-06-10-109
DIME Test ID: 2024-06-10-109-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2024-07-12

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: spaine
Date of test: 07/09/2024
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.08
Sample 1 Tear Strength: 182.5
Sample 2 Median Thickness: 0.077
Sample 2 Tear Strength: 194.1
Sample 3 Median Thickness: 0.078
Sample 3 Tear Strength: 212.3
UTM: 2kip
Median of the Tear Strength Values: 194.1 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point File
Test graph for Sample 3

Source: Bluehill Data Point File
Test graph for Sample 1

Source: Bluehill Data Point File
Test graph for Sample 2

Test was verified on 7/12/2024 ✔