Summary for Test 2017-06-13-7-3
Test performed: ASTM D624-00-re12Project Information
Project Identifiers | Project ID: 8196 DEA: 59912684 |
---|---|
DIST-CO-RTE-PM | 59--- |
Award Date | Not set |
Closeout Date | Not set |
Work Description | |
Location Description | |
QA Service Level | NOT VERIFIED |
Sample Information
Sample Taken Date | 06/13/2017 | Sample Unique Key | 7 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 06/15/2017 |
Sample type | Quality Assurance | A brief description of the sample | 2 Plain Bearing Pads |
The quantity of what the sample constitutes | 2 | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | Greg | Last name of sampler or witnessed by | Thompson |
Title of sampler | Unknown | Telephone number of sampler | Unknown |
Laboratory sample identification | Unknown | Linked DIME Sample ID | Unknown |
The fabricator/manufacturer/facility name | Warco Biltrite | Transportation Laboratory (TL) Number | C741428 |
Inspector Lot Number from the Transportation Laboratory (TL) Form | B902517 | Structure unique identifier | Not set |
Structure name | Not set |
Material Information
Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 05 16 16 1, 5 30 17 1 |
---|---|---|---|
Material/Compound/Elastomer ID | NA | Samples Representing | 59ft |
Description (size) | .375in x 48in x 180ft | Comments | Unknown |
Description (Number of Shims) | 0 | Type of Bearing Pad | Plain |
Description (Thickness of Shims) | NA | Manufacturer(s) | Warco Biltrite |
Batch Number | NA |
Test Details
DIME Sample ID: 2017-06-13-7
DIME Test ID: 2017-06-13-7-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-07-13
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 06/23/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.086 in
Sample 1 Tear Strength: 290.7 lbf / in
Sample 2 Median Thickness: 0.087 in
Sample 2 Tear Strength: 298.9 lbf / in
Sample 3 Median Thickness: 0.075 in
Sample 3 Tear Strength: 320 lbf / in
UTM: no data
Median of the Tear Strength Values: 298.9 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 7/6/2017 ✔