Summary for Test 2017-03-23-2-3
Test performed: ASTM D624-00-re12Project Information
| Project Identifiers | Project ID: 210828 DEA: 07290704 EFIS: 0712000076 |
|---|---|
| DIST-CO-RTE-PM | 07-LA-47-0.9/2.0 |
| Award Date | 04/06/2016 |
| Closeout Date | 06/25/2019 |
| Work Description | RESTORE BRIDGE SEISMIC. |
| Location Description | Not set |
| QA Service Level | 1 (Verified on 06/03/2016) |
Sample Information
| Sample Taken Date | 03/23/2017 | Sample Unique Key | 2 |
|---|---|---|---|
| Date that the sample was received by the laboratory/organization performing the testing | 03/24/2017 | Sample type | Quality Assurance |
| A brief description of the sample | elastomeric bearing pad | The quantity of what the sample constitutes | 11 |
| From where was the sample collected | Fabricator | First name of sampler or witnessed by | James |
| Last name of sampler or witnessed by | Doe | Title of sampler | Unknown |
| Telephone number of sampler | Unknown | Laboratory sample identification | Unknown |
| Linked DIME Sample ID | Unknown | The fabricator/manufacturer/facility name | Cal-Neva |
| Transportation Laboratory (TL) Number | Unknown | Inspector Lot Number from the Transportation Laboratory (TL) Form | B35801817 |
| Structure unique identifier | Not set | Structure name | Not set |
| Bid Item | Not set |
Material Information
| Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 02227262 |
|---|---|---|---|
| Material/Compound/Elastomer ID | 055E0507 | Samples Representing | 11 |
| Description (size) | .75 x 36 x 36 | Comments | Unknown |
| Description (Number of Shims) | 0 | Type of Bearing Pad | Plain |
| Description (Thickness of Shims) | NA | Manufacturer(s) | Warco Biltrite |
| Batch Number | 1111797 |
Test Details
DIME Sample ID: 2017-03-23-2
DIME Test ID: 2017-03-23-2-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-04-10
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 03/28/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.086 in
Sample 1 Tear Strength: 255.8 lbf / in
Sample 2 Median Thickness: 0.079 in
Sample 2 Tear Strength: 240.5 lbf / in
Sample 3 Median Thickness: 0.083 in
Sample 3 Tear Strength: 253 lbf / in
UTM: no data
Median of the Tear Strength Values: 253 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 4/3/2017 ✔