Summary for Test 2022-12-05-45-5

Test performed: ASTM D624-00r20

Project Information

Project IdentifiersProject ID: 993401
DEA: 11430494
EFIS: 1118000262
DIST-CO-RTE-PM11-IMP-8-R96.8
Award Date09/01/2022
Closeout Date02/28/2024
Work DescriptionREHABILITATE BRIDGE DECK, SLABS, BEARING PADS, JOINT SEALS & OVERLAY.
Location DescriptionIMPERIAL COUNTY NEAR WINTERHAVEN AT COLORADO RIVER VIADUCT BRIDGE NO. 58-0312 L/R
QA Service Level1 (Verified on 11/30/2021)

Sample Information

Sample Taken Date12/05/2022 Sample Unique Key45
Date that the sample was received by the laboratory/organization performing the testing12/19/2022 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes7
From where was the sample collectedFabricator First name of sampler or witnessed byNA
Last name of sampler or witnessed byNA Title of sampler
Telephone number of sampler Laboratory sample identification
Linked DIME Sample ID The fabricator/manufacturer/facility nameDynamic Rubber
Transportation Laboratory (TL) Number Inspector Lot Number from the Transportation Laboratory (TL) Form
Structure unique identifier Structure name
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)CR55-014-A
Material/Compound/Elastomer IDNA Samples Representing7
Description (size)4.60x17x42 Comments
Description (Number of Shims)8 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Dynamic Rubber
Batch Number273

Test Details

DIME Sample ID: 2022-12-05-45
DIME Test ID: 2022-12-05-45-5
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00r20: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2023-01-11

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: spaine
Date of test: 01/09/2023
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.073
Sample 1 Tear Strength: 208.8
Sample 2 Median Thickness: 0.077
Sample 2 Tear Strength: 204.8
Sample 3 Median Thickness: 0.074
Sample 3 Tear Strength: 202.3
UTM: 2kip
Median of the Tear Strength Values: 204.8 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point File
Test graph for Sample 3

Source: Bluehill Data Point File
Test graph for Sample 2

Source: Bluehill Data Point File
Test graph for Sample 1

Test was verified on 1/11/2023 ✔