Summary for Test 2016-09-07-6-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 210734
DEA: 043G4574
EFIS: 0412000057
DIST-CO-RTE-PM04-CC,MRN,SF-580,580,80-580PM6.1/7.8,0.0/2.6,80PM5.7/7.7
Award Date10/21/2015
Closeout Date01/03/2018
Work DescriptionREPLACE JOINT SEALS, CONSTRUCT APPROACH SLAB, REPAIR DECK DRAINS
Location DescriptionIN CONTRA COSTA, MARIN, AND SAN FRANCISCO COUNTIES ON THE SANFRANCISCO-OAKLAND BAY BRIDGE ANDRICHMOND -SAN RAFAEL BRIDGE
QA Service Level1 (Verified on 09/16/2015)

Sample Information

Sample Taken Date09/07/2016 Sample Unique Key6
Date that the sample was received by the laboratory/organization performing the testing09/22/2016 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes1
From where was the sample collectedManufacturer First name of sampler or witnessed byDavid
Last name of sampler or witnessed bySimon Title of samplerUnknown
Telephone number of samplerUnknown Laboratory sample identificationUnknown
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility nameD S Brown
Transportation Laboratory (TL) NumberNA Inspector Lot Number from the Transportation Laboratory (TL) FormNA
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)C1609-6071-24
Material/Compound/Elastomer IDNA Samples Representing83
Description (size).5in x 6in x 6in CommentsUnknown
Description (Number of Shims)0 Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)D S Brown
Batch NumberNA

Test Details

DIME Sample ID: 2016-09-07-6
DIME Test ID: 2016-09-07-6-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2016-09-29

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 09/22/2016
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.078 in
Sample 1 Tear Strength: 269.2 lbf / in
Sample 2 Median Thickness: 0.077 in
Sample 2 Tear Strength: 259.7 lbf / in
Sample 3 Median Thickness: 0.07 in
Sample 3 Tear Strength: 257.1 lbf / in
UTM: no data
Median of the Tear Strength Values: 259.7 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 9/29/2016 ✔