Summary for Test 2016-09-12-3-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 210735
DEA: 071193U4
EFIS: 0713000007
DIST-CO-RTE-PM07-LA-10-37.2/42.4
Award Date11/16/2015
Closeout Date07/11/2022
Work DescriptionCONSTRUCT HOV LANES, WIDEN BRIDGES, AND REALIGN RAMPS.
Location DescriptionIN LA COUNTY FROM CITRUS STREET IN WEST COVINA TO ROUTE 57 IN POMONA
QA Service Level1 (Verified on 03/07/2016)

Sample Information

Sample Taken Date09/12/2016 Sample Unique Key3
Date that the sample was received by the laboratory/organization performing the testing09/13/2016 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes2
From where was the sample collectedSource First name of sampler or witnessed byPete
Last name of sampler or witnessed byEtcheverry Title of samplerUnknown
Telephone number of samplerUnknown Laboratory sample identificationUnknown
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility nameScougal Rubber
Transportation Laboratory (TL) NumberUnknown Inspector Lot Number from the Transportation Laboratory (TL) FormUnknown
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)14757-1 4
Material/Compound/Elastomer IDNA Samples Representing2
Description (size)3in x 14in x 14in CommentsUnknown
Description (Number of Shims)6 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch NumberNA

Test Details

DIME Sample ID: 2016-09-12-3
DIME Test ID: 2016-09-12-3-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2016-09-20

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 09/16/2016
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.076 in
Sample 1 Tear Strength: 263.2 lbf / in
Sample 2 Median Thickness: 0.07 in
Sample 2 Tear Strength: 242.9 lbf / in
Sample 3 Median Thickness: 0.066 in
Sample 3 Tear Strength: 272.7 lbf / in
UTM: no data
Median of the Tear Strength Values: 263.2 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 9/20/2016 ✔