Summary for Test 2016-02-08-4-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 209059
DEA: 033E1004
EFIS: 0300000473
DIST-CO-RTE-PM03-PLA-80-8.1/37.8
Award Date01/28/2014
Closeout Date01/23/2017
Work DescriptionIMPROVING VERTICAL CLEARANCE
Location DescriptionPLACER COUNTY IN AND NEAR LOOMIS, PENRYN, NEWCASTLE, WEIMAR, AND MAGRA FROM 0.1 MILE WEST OF BRACE ROAD OVERCROSSING TO 0.1 MILE EAST OF MAGRA OVERCROSSING
QA Service Level1 (Verified on 01/15/2014)

Sample Information

Sample Taken Date02/08/2016 Sample Unique Key4
Date that the sample was received by the laboratory/organization performing the testing02/10/2016 Sample typeQuality Assurance
A brief description of the sampleBearing Pad The quantity of what the sample constitutes11
From where was the sample collectedFabricator First name of sampler or witnessed byPete
Last name of sampler or witnessed byEtcheverry Title of samplerUnknown
Telephone number of samplerUnknown Laboratory sample identificationUnknown
Linked DIME Sample IDUnknown The fabricator/manufacturer/facility namescougal
Transportation Laboratory (TL) NumberUnknown Inspector Lot Number from the Transportation Laboratory (TL) FormUnknown
Structure unique identifierNot set Structure nameNot set
Bid ItemNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)14186-1
Material/Compound/Elastomer IDNA Samples Representing11
Description (size)3in x 10in x 10in CommentsUnknown
Description (Number of Shims)5 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal
Batch NumberNA

Test Details

DIME Sample ID: 2016-02-08-4
DIME Test ID: 2016-02-08-4-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2016-02-23

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 02/12/2016
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.076 in
Sample 1 Tear Strength: 250 lbf / in
Sample 2 Median Thickness: 0.07 in
Sample 2 Tear Strength: 242.9 lbf / in
Sample 3 Median Thickness: 0.073 in
Sample 3 Tear Strength: 232.9 lbf / in
UTM: 2KIP
Median of the Tear Strength Values: 242.9 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 2/23/2016 ✔