Summary for Test 2021-02-09-28-7
Test performed: ASTM D2628-91-re16Project Information
Project Identifiers | Project ID: 88888 DEA: SMTL-STOCK EFIS: SMTL-STOCK |
---|---|
DIST-CO-RTE-PM | 59--- |
Award Date | Not set |
Closeout Date | Not set |
Work Description | Special project for SMTL stock material. Object Code: 1025. J2 DEA: 912680. |
Location Description | Not set |
QA Service Level | NOT VERIFIED |
Sample Information
Sample Taken Date | 02/09/2021 | Sample Unique Key | 28 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 02/05/2021 |
Sample type | Quality Assurance | A brief description of the sample | Joint Seal |
The quantity of what the sample constitutes | 550' | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | David | Last name of sampler or witnessed by | Simon |
Title of sampler | Telephone number of sampler | ||
Laboratory sample identification | Linked DIME Sample ID | ||
The fabricator/manufacturer/facility name | Watson Bowman | Transportation Laboratory (TL) Number | |
Inspector Lot Number from the Transportation Laboratory (TL) Form | Structure unique identifier | ||
Structure name |
Material Information
Material Type | SMTL TM2 - Type B Elastomeric Joint Seal | Mfg. Lot Number(s) | 0221128 |
---|---|---|---|
Manufacturer(s) | Watson Bowman | Temperature | 72 |
Humidity | 50 | Comments | |
Joint Seal Size | 3.75" |
Test Details
DIME Sample ID: 2021-02-09-28
DIME Test ID: 2021-02-09-28-7
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D2628-91-re16: Standard Specification for Preformed Polychloroprene Elastomeric Joint Seals for Concrete Pavements
Test Release Date: 2021-03-16
Test Results
Input Type: Measured
Tester's full name: Steven Paine
Date of test: 03/02/2021
High or low tempurature: High
Temperature: 72 f
Humidity: 50 %
Temp Recovery (22 hrs at -20F) Size Before (Height of Contact Face ): 3.75 in
Temp Recovery (22 hrs at -20F) Size After (Recovered Contact Face ): 3.75 in
Percent Recovery: 100 %
General comments (publicly viewable) (Max 1000 characters):
Test was verified on 3/16/2021 ✔