Summary for Test 2018-09-06-7-4

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 210837
DEA: 080J0804
EFIS: 0800000283
COOP: 081625
DIST-CO-RTE-PM08-RIV-15-34.7/51.6
Award Date04/17/2017
Closeout DateNot set
Work Description(Alternative Delivery) DESIGN-BUILD OF THE INTERSTATE 15 EXPRESS LANES PROJECT
Location DescriptionRiverside County and SBD-15-0.0/1.3
QA Service Level1 (Verified on 05/08/2017)

Sample Information

Sample Taken Date09/06/2018 Sample Unique Key7
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing09/12/2018
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes1 From where was the sample collectedManufacturer
First name of sampler or witnessed byPete Last name of sampler or witnessed byEtcheverry
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameScougal Rubber Transportation Laboratory (TL) NumberNA
Inspector Lot Number from the Transportation Laboratory (TL) FormNA Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)16841-3, 4, 5, 6, 7, 8, 9, 10, 11
Material/Compound/Elastomer IDNA Samples Representing14
Description (size)4" x 18" x 18" CommentsUnknown
Description (Number of Shims)8 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch NumberNA

Test Details

DIME Sample ID: 2018-09-06-7
DIME Test ID: 2018-09-06-7-4
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2018-10-03

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 09/19/2018
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.068 in
Sample 1 Tear Strength: 205.9 lbf / in
Sample 2 Median Thickness: 0.065 in
Sample 2 Tear Strength: 200 lbf / in
Sample 3 Median Thickness: 0.062 in
Sample 3 Tear Strength: 193.5 lbf / in
UTM: no data
Median of the Tear Strength Values: 200 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 9/26/2018