Summary for Test 2018-01-29-5-2
Test performed: ASTM D2628-91-re11-lowProject Information
Project Identifiers | Project ID: 88888 DEA: SMTL-STOCK EFIS: SMTL-STOCK |
---|---|
DIST-CO-RTE-PM | 59--- |
Award Date | Not set |
Closeout Date | Not set |
Work Description | Special project for SMTL stock material. Object Code: 1025. J2 DEA: 912680. |
Location Description | Not set |
QA Service Level | NOT VERIFIED |
Sample Information
Sample Taken Date | 01/29/2018 | Sample Unique Key | 5 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 01/31/2018 |
Sample type | Quality Assurance | A brief description of the sample | Joint Seal |
The quantity of what the sample constitutes | 500ft | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | David | Last name of sampler or witnessed by | Simon |
Title of sampler | Unknown | Telephone number of sampler | Unknown |
Laboratory sample identification | Unknown | Linked DIME Sample ID | Unknown |
The fabricator/manufacturer/facility name | Watson Bowman | Transportation Laboratory (TL) Number | NA |
Inspector Lot Number from the Transportation Laboratory (TL) Form | NA | Structure unique identifier | Not set |
Structure name | Not set |
Material Information
Material Type | SMTL TM2 - Type B Elastomeric Joint Seal | Mfg. Lot Number(s) | 0618123 |
---|---|---|---|
Manufacturer(s) | Watson Bowman | Temperature | 72 |
Humidity | 50 | Comments | Unknown |
Joint Seal Size | 2.75 |
Test Details
DIME Sample ID: 2018-01-29-5
DIME Test ID: 2018-01-29-5-2
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D2628-91-re11-low: Standard Specification for Preformed Polychloroprene Elastomeric Joint Seals for Concrete Pavements (Low Temp Recovery)
Test Release Date: 2018-02-27
Test Results
Input Type: Measured
Tester's full name: Randy Kattenhorn
Date of test: 02/06/2018
Temperature: 72 f
Humidity: 50 %
Low Temp Recovery (22 hrs at -20F) Size Before (Height of Contact Face ): 2.75 in
Low Temp Recovery (22 hrs at -20F) Size After (Recovered Contact Face ): 2.41 in
Percent Recovery (Low Temp): 88 %
General comments (publicly viewable) (Max 1000 characters):
Test was verified on 2/20/2018 ✔