Summary for Test 2017-10-10-5-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 209146
DEA: 06471504
EFIS: 0600000464
COOP: 061549
DIST-CO-RTE-PM06-TUL-99-39.6/41.3
Award Date02/24/2017
Closeout Date03/03/2020
Work DescriptionRECONSTRUCT INTERCHANGE WITH NEW PUMPING PLANT.
Location DescriptionTULARE COUNTY AT GOSHEN FROM 0.9 MILE NORTH OF ROUTE 99/198 WEST SEPARATION TO 0.2 MILE NORTH OF NORTH GOSHEN OVERHEAD
QA Service Level1 (Verified on 10/08/2013)

Sample Information

Sample Taken Date10/10/2017 Sample Unique Key5
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing10/10/2017
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes1 From where was the sample collectedManufacturer
First name of sampler or witnessed byRob Last name of sampler or witnessed byAnderson
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameScougal Rubber Transportation Laboratory (TL) NumberNA
Inspector Lot Number from the Transportation Laboratory (TL) FormNA Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)16038-1
Material/Compound/Elastomer IDNA Samples Representing27
Description (size)2.5" x 14" x 16" CommentsUnknown
Description (Number of Shims)5 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch NumberNA

Test Details

DIME Sample ID: 2017-10-10-5
DIME Test ID: 2017-10-10-5-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-10-19

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 10/11/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.073 in
Sample 1 Tear Strength: 232.9 lbf / in
Sample 2 Median Thickness: 0.074 in
Sample 2 Tear Strength: 216.2 lbf / in
Sample 3 Median Thickness: 0.072 in
Sample 3 Tear Strength: 236.1 lbf / in
UTM: no data
Median of the Tear Strength Values: 232.9 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 10/12/2017