Summary for Test 2017-01-24-2-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 211668
DEA: 010B2604
EFIS: 0112000150
DIST-CO-RTE-PM01-DN-199-8.2
Award Date11/07/2016
Closeout Date01/07/2019
Work DescriptionCONSTRUCT BRIDGE AND WIDEN SHOULDERS
Location DescriptionDEL NORTE COUNTY NEAR HIOUCHI AT 1 MILE NORTH OF SOUTH FORK ROAD
QA Service Level1 (Verified on 09/27/2016)

Sample Information

Sample Taken Date01/24/2017 Sample Unique Key2
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing01/24/2017
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes2 From where was the sample collectedManufacturer
First name of sampler or witnessed byRob Last name of sampler or witnessed byAnderson
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameScougal Rubber Transportation Laboratory (TL) NumberNA
Inspector Lot Number from the Transportation Laboratory (TL) FormNA Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)15480-1,2
Material/Compound/Elastomer IDNA Samples Representing2
Description (size)3" x 12" x 12" CommentsUnknown
Description (Number of Shims)6 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Scougal Rubber
Batch NumberNA

Test Details

DIME Sample ID: 2017-01-24-2
DIME Test ID: 2017-01-24-2-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-02-09

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 01/27/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.078 in
Sample 1 Tear Strength: 256.4 lbf / in
Sample 2 Median Thickness: 0.083 in
Sample 2 Tear Strength: 241 lbf / in
Sample 3 Median Thickness: 0.076 in
Sample 3 Tear Strength: 250 lbf / in
UTM: no data
Median of the Tear Strength Values: 250 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 2/2/2017