Summary for Test 2016-06-27-8-13

Test performed: CTM 670-December 2013

Project Information

Project IdentifiersProject ID: 8196
DEA: 59912684
DIST-CO-RTE-PM59---
Award DateNot set
Closeout DateNot set
Work Description
Location Description
QA Service LevelNOT VERIFIED

Sample Information

Sample Taken Date06/27/2016 Sample Unique Key8
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing07/04/2016
Sample typeAuthorization A brief description of the sampleHY Ten Coupler
The quantity of what the sample constitutes12 From where was the sample collectedManufacturer
First name of sampler or witnessed byRichard Last name of sampler or witnessed byWebster
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameHY Ten Reinforcement Transportation Laboratory (TL) NumberNA
Inspector Lot Number from the Transportation Laboratory (TL) FormNA Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM5 - Couplers Production or Authorization TestingAuthorization Testing
Service or UltimateUltimate Material Standard CodeASTM A706
Material Grade60 Rebar ManufacturerHY Ten
Coupler ManufacturerHY Ten Intermediate Assembler or FabricatorUnknown
Rebar Size#4, 5, 6, 8, 14 Coupler ModelHTS HTP HTL
Coating StandardsUncoated Shape of RebarStraight
Rebar Hoop DiameterUnknown Rebar Hoop FabricatorUnknown
Coupler Component Heat/Lot Number(s)4, 5, 6, 8, 14, HTS, HTP, HTL Rebar Heat Number(s)4049941, 4051049, 4048405, 4050513, 3055577
Rebar Size 2 NA Coupler Unique IDNot set

Test Details

DIME Sample ID: 2016-06-27-8
DIME Test ID: 2016-06-27-8-13
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: CTM 670-December 2013: Method of Tests for Mechanical and Welded Reinforcing Steel Splices (Cyclical/Fatique Tensile with Slip)
Test Release Date: 2017-01-27

Test Results


Number of Samples Tested: 1
Input Type: Measured
Tester's full name: Fred
Date of test: 01/13/2017
UTM: 2000KIP
Temperature: 72 F
Halo ID: Big
NumSampleNumber of CyclesSizeMfg. Lot Number(s)Slip (inch)Area (sqin)Peak Load (lbf)Peak Stress (psi)CommentsTested By
1210000#14/43mmHTP02.2521706796474Broke in Heat Affected Zone At WeldFred

General comments (publicly viewable) (Max 1000 characters): Broke in Heat Affected Zone At Weld; NO Necking
Test Graph
WARNING: No graph data imported from Instron machine.

Test was verified on 1/20/2017