Summary for Test 2020-11-18-28-4

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 214114
DEA: 040A5394
EFIS: 0418000244
DIST-CO-RTE-PM04-SOL-80,12-11.4/12.8, 2.1/2.8
Award DateNot set
Closeout Date02/24/2023
Work DescriptionWiden EB SR-12 Connector, Construct 3 ramps & 2 box girder bridges, remove existing bridge, etc.
Location DescriptionI-80/I-680/Route 12 Interchange
QA Service Level1 (Verified on 04/23/2019)

Sample Information

Sample Taken Date11/18/2020 Sample Unique Key28
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing11/30/2020
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes2 From where was the sample collectedManufacturer
First name of sampler or witnessed byKayla Last name of sampler or witnessed byWallace
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameDynamic Rubber Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifier
Structure name

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)CR55-027-20
Material/Compound/Elastomer IDna Samples Representing92
Description (size)1"x4"x6" Comments
Description (Number of Shims)0 Type of Bearing PadPlain
Description (Thickness of Shims)NA Manufacturer(s)Dynamic Rubber
Batch Numberna

Test Details

DIME Sample ID: 2020-11-18-28
DIME Test ID: 2020-11-18-28-4
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2020-12-14

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: spaine
Date of test: 12/10/2020
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.075
Sample 1 Tear Strength: 272.1
Sample 2 Median Thickness: 0.083
Sample 2 Tear Strength: 259.8
Sample 3 Median Thickness: 0.072
Sample 3 Tear Strength: 301.9
UTM: 2kip
Median of the Tear Strength Values: 272.1 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point File
Test graph for Sample 1

Source: Bluehill Data Point File
Test graph for Sample 2

Source: Bluehill Data Point File
Test graph for Sample 3

Test was verified on 12/14/2020