Summary for Test 2020-08-24-10-3
Test performed: ASTM D624-00-re12Project Information
Project Identifiers | Project ID: 214791 DEA: 112N0544 EFIS: 1118000268 |
---|---|
DIST-CO-RTE-PM | 11-SD-5,15,54,75,94,805-Var |
Award Date | 05/26/2020 |
Closeout Date | 01/31/2022 |
Work Description | METHACRYLATE BRIDGE DECK, REPAIR SPALLS & REPLACE JOINTS SEALS. |
Location Description | SAN DIEGO COUNTY AT VARIOUS LOCATIONS |
QA Service Level | 1 (Verified on 07/29/2020) |
Sample Information
Sample Taken Date | 08/24/2020 | Sample Unique Key | 10 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 08/27/2020 |
Sample type | Quality Assurance | A brief description of the sample | Bearing Pad |
The quantity of what the sample constitutes | 1 | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | Kayla | Last name of sampler or witnessed by | Wallace |
Title of sampler | Telephone number of sampler | ||
Laboratory sample identification | Linked DIME Sample ID | ||
The fabricator/manufacturer/facility name | Dynamic Rubber | Transportation Laboratory (TL) Number | |
Inspector Lot Number from the Transportation Laboratory (TL) Form | Structure unique identifier | ||
Structure name |
Material Information
Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 16164 |
---|---|---|---|
Material/Compound/Elastomer ID | na | Samples Representing | 5 |
Description (size) | 2.30"x16"x22" | Comments | |
Description (Number of Shims) | 4 | Type of Bearing Pad | Steel |
Description (Thickness of Shims) | 14 gage | Manufacturer(s) | Dynamic Rubber |
Batch Number | na |
Test Details
DIME Sample ID: 2020-08-24-10
DIME Test ID: 2020-08-24-10-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2020-09-14
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: spaine
Date of test: 08/28/2020
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.081
Sample 1 Tear Strength: 232.7
Sample 2 Median Thickness: 0.077
Sample 2 Tear Strength: 242.9
Sample 3 Median Thickness: 0.071
Sample 3 Tear Strength: 263.3
UTM: 2kip
Median of the Tear Strength Values: 242.9 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point FileTest graph for Sample 3
Source: Bluehill Data Point File
Test graph for Sample 1
Source: Bluehill Data Point File
Test graph for Sample 2
Test was verified on 9/14/2020 ✔