Summary for Test 2020-05-20-10-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 214515
DEA: 024F6004
EFIS: 0213000012
DIST-CO-RTE-PM02-SIS,TRI-36,96,299-VAR
Award Date01/14/2020
Closeout Date08/24/2022
Work DescriptionBRIDGE DECK REPAIR, POLYESTER OVERLAY AND RAIL REPLACEMENT.
Location DescriptionSISKIYOU AND TRINITY COUNTIES AT VARIOUS LOCATIONS
QA Service Level1 (Verified on 01/22/2020)

Sample Information

Sample Taken Date05/20/2020 Sample Unique Key10
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing05/22/2020
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes24 From where was the sample collectedManufacturer
First name of sampler or witnessed byKayla Last name of sampler or witnessed byWallace
Title of sampler Telephone number of sampler
Laboratory sample identification Linked DIME Sample ID
The fabricator/manufacturer/facility nameDynamic Rubber Transportation Laboratory (TL) Number
Inspector Lot Number from the Transportation Laboratory (TL) Form Structure unique identifier
Structure name

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)CR55-008-20
Material/Compound/Elastomer IDNA Samples Representing1
Description (size)5.18 x 20 x 26 CommentsUnknown
Description (Number of Shims)6 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Dynamic Rubber
Batch Number224

Test Details

DIME Sample ID: 2020-05-20-10
DIME Test ID: 2020-05-20-10-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2020-05-28

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: bewing
Date of test: 05/27/2020
Humidity: 50.00 %
Temperature: 72 F
Sample 1 Median Thickness: 0.09
Sample 1 Tear Strength: 200.9
Sample 2 Median Thickness: 0.081
Sample 2 Tear Strength: 215.3
Sample 3 Median Thickness: 0.089
Sample 3 Tear Strength: 200.2
UTM: 2kip
Median of the Tear Strength Values: 200.9 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Bluehill Data Point File
Test graph for Sample 3

Source: Bluehill Data Point File
Test graph for Sample 2

Source: Bluehill Data Point File
Test graph for Sample 1

Test was verified on 5/28/2020