Summary for Test 2018-09-25-6-4

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 213213
DEA: 030G8004
EFIS: 0316000246
DIST-CO-RTE-PM03-COL,GLE,SAC,SUT,YUB-5,20,65,80,99-VAR
Award Date05/10/2018
Closeout Date12/04/2019
Work DescriptionREMOVE AC, PLACE METHACRYLATE & REPAIR BRIDGE JOINTS ON 9 BRIDGES
Location DescriptionCOLUSA, GLENN, SACRAMENTO, SUTTER, AND YUBA COUNTIES AT VARIOUS LOCATIONS
QA Service Level1 (Verified on 09/24/2018)

Sample Information

Sample Taken Date09/25/2018 Sample Unique Key6
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing09/28/2018
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes1 From where was the sample collectedManufacturer
First name of sampler or witnessed byMike Last name of sampler or witnessed bySpellman
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameDS Brown Seismic Energy Transportation Laboratory (TL) NumberNA
Inspector Lot Number from the Transportation Laboratory (TL) FormNA Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)4000713-1A
Material/Compound/Elastomer IDNA Samples Representing1
Description (size)1.724" x 12" x 19" CommentsUnknown
Description (Number of Shims)3 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)DS Brown
Batch NumberNA

Test Details

DIME Sample ID: 2018-09-25-6
DIME Test ID: 2018-09-25-6-4
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2018-10-23

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 10/05/2018
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.067 in
Sample 1 Tear Strength: 253.7 lbf / in
Sample 2 Median Thickness: 0.07 in
Sample 2 Tear Strength: 285.7 lbf / in
Sample 3 Median Thickness: 0.071 in
Sample 3 Tear Strength: 267.6 lbf / in
UTM: no data
Median of the Tear Strength Values: 267.6 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 10/16/2018