Summary for Test 2017-11-20-2-3
Test performed: ASTM D624-00-re12Project Information
Project Identifiers | Project ID: 211931 DEA: 043G6414 EFIS: 0416000348 |
---|---|
DIST-CO-RTE-PM | 04-NAP-29-37.0 |
Award Date | 03/17/2017 |
Closeout Date | 04/22/2020 |
Work Description | SCOUR REPLACE BRIDGE |
Location Description | NAPA COUNTY IN CALISTOGA AT NAPA RIVER BRIDGE |
QA Service Level | 1 (Verified on 02/15/2017) |
Sample Information
Sample Taken Date | 11/20/2017 | Sample Unique Key | 2 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | Yes | Date that the sample was received by the laboratory/organization performing the testing | 11/20/2017 |
Sample type | Quality Assurance | A brief description of the sample | Bearing Pad |
The quantity of what the sample constitutes | 1 | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | Pamela | Last name of sampler or witnessed by | Hagnice |
Title of sampler | Unknown | Telephone number of sampler | Unknown |
Laboratory sample identification | Unknown | Linked DIME Sample ID | Unknown |
The fabricator/manufacturer/facility name | Scougal Rubber | Transportation Laboratory (TL) Number | C882752 |
Inspector Lot Number from the Transportation Laboratory (TL) Form | NA | Structure unique identifier | Not set |
Structure name | Not set |
Material Information
Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 15732-1 |
---|---|---|---|
Material/Compound/Elastomer ID | NA | Samples Representing | 35 |
Description (size) | .5" x 12" x 48" | Comments | Unknown |
Description (Number of Shims) | 0 | Type of Bearing Pad | Plain |
Description (Thickness of Shims) | NA | Manufacturer(s) | Scougal Rubber |
Batch Number | NA |
Test Details
DIME Sample ID: 2017-11-20-2
DIME Test ID: 2017-11-20-2-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-11-28
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 11/20/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.08 in
Sample 1 Tear Strength: 262.5 lbf / in
Sample 2 Median Thickness: 0.068 in
Sample 2 Tear Strength: 264.7 lbf / in
Sample 3 Median Thickness: 0.078 in
Sample 3 Tear Strength: 269.2 lbf / in
UTM: no data
Median of the Tear Strength Values: 264.7 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 11/21/2017 ✔