Summary for Test 2017-07-21-4-3
Test performed: ASTM D624-00-re12Project Information
Project Identifiers | Project ID: 212222 DEA: 033H1004 |
---|---|
DIST-CO-RTE-PM | 03-ED-50-37.6, 37.60 |
Award Date | 03/16/2017 |
Closeout Date | 01/09/2019 |
Work Description | Construct Soldier Pile Wall |
Location Description | Not set |
QA Service Level | 1 (Verified on 06/19/2017) |
Sample Information
Sample Taken Date | 07/21/2017 | Sample Unique Key | 4 |
---|---|---|---|
Will the laboratory/organization for which you are a member perform testing on this material sample? | No | Date that the sample was received by the laboratory/organization performing the testing | 07/25/2017 |
Sample type | Acceptance | A brief description of the sample | 1x8x12 Steel Reinforced |
The quantity of what the sample constitutes | 63 | From where was the sample collected | Manufacturer |
First name of sampler or witnessed by | Kevin | Last name of sampler or witnessed by | Muser |
Title of sampler | QA | Telephone number of sampler | 916-517-0532 |
Laboratory sample identification | Linked DIME Sample ID | ||
The fabricator/manufacturer/facility name | Scougal Rubber | Transportation Laboratory (TL) Number | |
Inspector Lot Number from the Transportation Laboratory (TL) Form | S19-408-17 | Structure unique identifier | Not set |
Structure name | Not set |
Material Information
Material Type | SMTL TM1 - Elastomeric Bearing Pad | Mfg. Lot Number(s) | 179747V |
---|---|---|---|
Material/Compound/Elastomer ID | cp2527v55duroneogr3 | Samples Representing | 63 |
Description (size) | 1x8x12 | Comments | |
Description (Number of Shims) | 2 | Type of Bearing Pad | Steel |
Description (Thickness of Shims) | 14 gage | Manufacturer(s) | Scougal Rubber |
Batch Number | 16005 |
Test Details
DIME Sample ID: 2017-07-21-4
DIME Test ID: 2017-07-21-4-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2017-08-03
Test Results
Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 07/25/2017
Humidity: 50 %
Temperature: 72 F
Sample 1 Median Thickness: 0.066 in
Sample 1 Tear Strength: 227.3 lbf / in
Sample 2 Median Thickness: 0.064 in
Sample 2 Tear Strength: 187.5 lbf / in
Sample 3 Median Thickness: 0.064 in
Sample 3 Tear Strength: 187.5 lbf / in
UTM: no data
Median of the Tear Strength Values: 187.5 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point FileTest graph for Sample 1
Source: Partner Data Point File
Test graph for Sample 2
Source: Partner Data Point File
Test graph for Sample 3
Test was verified on 7/27/2017 ✔