Summary for Test 2016-08-12-11-3

Test performed: ASTM D624-00-re12

Project Information

Project IdentifiersProject ID: 211221
DEA: 010A1004
EFIS: 0112000023
DIST-CO-RTE-PM01-DN-101-VAR
Award Date04/28/2016
Closeout Date10/30/2017
Work DescriptionBRIDGE SEISMIC RETROFIT AND CLEAN AND PAINT BRIDGE.
Location DescriptionDEL NORTE COUNTY AT VARIOUS LOCATIONS
QA Service Level1 (Verified on 03/28/2016)

Sample Information

Sample Taken Date08/12/2016 Sample Unique Key11
Will the laboratory/organization for which you are a member perform testing on this material sample?Yes Date that the sample was received by the laboratory/organization performing the testing08/15/2016
Sample typeQuality Assurance A brief description of the sampleBearing Pad
The quantity of what the sample constitutes1 From where was the sample collectedDistributor
First name of sampler or witnessed byEd Last name of sampler or witnessed byFleming
Title of samplerUnknown Telephone number of samplerUnknown
Laboratory sample identificationUnknown Linked DIME Sample IDUnknown
The fabricator/manufacturer/facility nameDynatect Transportation Laboratory (TL) NumberC740864
Inspector Lot Number from the Transportation Laboratory (TL) FormB1025016 Structure unique identifierNot set
Structure nameNot set

Material Information

Material TypeSMTL TM1 - Elastomeric Bearing Pad Mfg. Lot Number(s)071916
Material/Compound/Elastomer ID340313 Samples Representing13
Description (size)2in x 4in x 6in CommentsUnknown
Description (Number of Shims)4 Type of Bearing PadSteel
Description (Thickness of Shims)14 gage Manufacturer(s)Dynatect
Batch NumberRL305502

Test Details

DIME Sample ID: 2016-08-12-11
DIME Test ID: 2016-08-12-11-3
Testing Lab: CT HQ - Sacramento Structural Materials Testing Laboratory
Test Method: ASTM D624-00-re12: Standard Test Method for Tear Strength of Conventional Vulcanized Rubber and Thermoplastic Elastomers
Test Release Date: 2016-08-31

Test Results


Number of specimens tested: 3
Input Type: Measured
Tester's full name: Brian
Date of test: 08/25/2016
Humidity: 50 %
Temperature: 71 F
Sample 1 Median Thickness: 0.072 in
Sample 1 Tear Strength: 250 lbf / in
Sample 2 Median Thickness: 0.076 in
Sample 2 Tear Strength: 263.2 lbf / in
Sample 3 Median Thickness: 0.078 in
Sample 3 Tear Strength: 256.4 lbf / in
UTM: no data
Median of the Tear Strength Values: 256.4 lb/in
General comments (publicly viewable) (Max 1000 characters):
Test Graph
Source: Partner Data Point File
Test graph for Sample 1

Source: Partner Data Point File
Test graph for Sample 2

Source: Partner Data Point File
Test graph for Sample 3

Test was verified on 8/31/2016