Note: Fields with no data or with a value of "Unknown" will not be displayed on the print out.
Project ID: 209694 DEA: 080J0704 EFIS: 0800000282
QA Service Level: 1
DIST-CO-RTE-PM: 08-SBD-215-0.6/1.7
Work Description: (Alternative Delivery) The CMGC project will reconstruct and improve interchange of I-215 and Barton Road in the City of Grand Terrace, CA.
Location Description: Grade separation at Intersection of I-215 and Barton Road near Grand Terrace, CA. ? On I-215 between I-10 and SR-60.
Contractor Name: Myers / Rados-Southern California Jobsite Office
Contractor Address: 12210 Michigan St., Suite D, Grand Terrace, CA 92313
Resident Engineer: Fereydoon Alipanah Structure Rep.: Tim Flores
DIME Sample ID: 2019-02-18-5
TL Number from the TL Form:
Sample Submitted By Organization: CT D08 - Fontana Southern Regional Laboratory
Sample Organization Contact: 213-792-4794
Type of Sample: Acceptance
Type of Material: Hot Mix Asphalt
Sample Taken Date: 02/18/2019
Date that the sample was received by the laboratory/organization performing the testing: 02/25/2019
The quantity of what the sample constitutes: 2 boxes 817.82 tons out
A brief description of the sample: 3/4" HMA-A R15 PG 64-28M 0.5 LAS
From where was the sample collected: Source
Laboratory sample identification: Lab 0142-19
Structure unique identifier:
Structure name:
The fabricator/manufacturer/facility name: Vulcan Corona
DIME Test ID: 2019-02-18-5-1
Test Method: AASHTO T308-10: Standard Method of Test for Determining the Asphalt Binder Content of Hot Mix Asphalt (HMA) by the Ignition Method (Method A) (Asphalt Binder Content)
Verified Date: 02/27/2019
Date Tested: 02/26/2019
Submitted By Organization: CT D08 - Fontana Southern Regional Laboratory
Organization Address: 13970 Victoria Street,
Organization City: Fontana
Organization State: CA
Organization Zipcode: 92336
Organization Email: jose.guzman@dot.ca.gov
Organization Phone: 9098293029
General Comments for this Test:
Test Result Compliance: complies
Additional Comments When Verified:
What temperature unit is used?
|
Fahrenheit
|
Test procedure used?
|
Method A
|
Mass of HMA Sample prior to ignition
|
no data
|
Corrected Asphalt Binder Content
|
4.65 %
|
Mass Loss
|
no data
|
Correction Factor (Percent by mass of HMA Specimen)
|
no data
|
Moisture Content
|
no data
|
Temperature Compensation Factor
|
no data
|
Test Temperature
|
no data
|