| Number of Cores | 2 |
| Core ID | 6A74 |
| Dry Weight | 947.7 grams |
| Parrafin Coated Weight | 965.4 grams |
| Coated Weight in Water | 530 grams |
| Theoretical Maximum Density | 2.389 |
| Core 2 ID | 6B74 |
| Dry Weight 2 | 935.5 grams |
| Parrafin Coated Weight 2 | 955.4 grams |
| Coated Weight in Water 2 | 520.2 grams |
| What temperature unit is used? | Fahrenheit |
| Test procedure used? | Method A |
| Mass of the specimen basket assembly | 3925.4 g |
| Mass of the specimen and specimen basket assembly prior to ignition | 5969.6 g |
| Mass of HMA Sample prior to ignition | 2044.2 g |
| Corrected Asphalt Binder Content | 8.68 % |
| Mass Loss | 188.5 g |
| Mass of aggregate remaining after ignition | 1855.7 g |
| Correction Factor (Percent by mass of HMA Specimen) | 0.54 % |
| Moisture Content | no data0 % |
| Temperature Compensation Factor | no data0 % |
| Test Temperature | 538 F |
| Number of tests | 1 |
| What is the unit of measurement for theoretical density? | US Units |
| Mass Determination | Air |
| Method Performed | Mechanical Agitation - Method A |
| Mass of container filled with water | 7475.6 grams |
| Mass of oven-dry sample in air for Sample 1 | 2517.2 grams |
| Mass of container filled with the sample and water for Sample 1 | 8939.1 grams |
| Temperature of Water | 77 °F |
| Specific Gravity for Sample 1 | 2.389 |
| Theoretical maximum density at 25°C (77°F) | 148.7 lb/ft^3 |
| What temperature unit is used? | Celsius |
| Test procedure used? | Method A |
| Mass of the specimen basket assembly | 4028.5 g |
| Mass of the specimen and specimen basket assembly prior to ignition | 6052.5 g |
| Corrected Asphalt Binder Content | 8.41 % |
| Mass of HMA Sample prior to ignition | 2024 g |
| Mass Loss | 179.8 g |
| Mass of aggregate remaining after ignition | 1844.2 g |
| Correction Factor (Percent by mass of HMA Specimen) | 0.47 % |
| Moisture Content | no data0 % |
| Temperature Compensation Factor | no data0 % |
| Test Temperature | 538 C |